Glass Lid , Cookware Parts of Tempered Glass Fry Pan Lid

China Glass Lid, Cookware Parts of Tempered Glass Fry Pan Lid, Find details and Price about China Glass Lid, Tempered Glass Lid from Glass Lid, Cookware Parts of Tempered Glass Fry Pan Lid

Model NO.
C-TYPE
Trademark
Meanco
Transport Package
Inner Packing: Lined with Alikali Paper,
Specification
Outer pakcing: 5 ply-corrugated cartons
Origin
Made in China
HS Code
7010200000
Model NO.
C-TYPE
Trademark
Meanco
Transport Package
Inner Packing: Lined with Alikali Paper,
Specification
Outer pakcing: 5 ply-corrugated cartons
Origin
Made in China
HS Code
7010200000
  • Material of tempered glass lid: Float glass              
  • Optional stainless steel rim: SUS201, SUS202, SUS301, SUS304             
  • Diameter: 10-50cm (Max. Dia. 50cm for round type, Max. Diagonal line length 45cm for square or rectangular lid )
  • Thickness: 4mm or 5mm            
  • Heat resistance: 320 degree centigrade              
  • Thermal shock: 180 degree centigrade              
  • Break-resistance: Five times of normal glass             
  • Excellent transparency allows for checking on cooking food at a glance              
  • Shape: Square, round, oval, rectangle 
  • Colors: Clear, blue, green, brown, etc.
  • Optional steam vent, logos and decorations.
  • Dishwasher safe for easy clean up
  • Delivery time 20-30 days after sample and order confirmation (20'FLC)
  • Sample Terms: Samples are available upon receipt of your requests
  • Package detail: Inner packing: Lined with Alikali paper, Outer pakcing: 5 ply-corrugated cartons
Glass Lid, Cookware Parts of Tempered Glass Fry Pan Lid
Glass Lid, Cookware Parts of Tempered Glass Fry Pan LidGlass Lid, Cookware Parts of Tempered Glass Fry Pan Lid
Test for quality control: 
 
1. FLATNESS CHECK
Place the glass lid on a completely smooth table , and put a piece of 1mm thickness iron plate beside the ring the glass lid, then moving the iron gauge along with the circumference of the lid, the glass lid passes the test if the iron plate does not push in
 
2. THTERMAL SHOCK
Put the glass lid into oven temperature to 200°C, and constant temperature for 30 minutes, remove it immediately into 20°C water , glass no broken or crack
 
3. IMPACT TEST
Place a lid, domed size up, on a hard surface,
Dropping a 225 grams steel ball from a height of 1.5meter,
No fracture no shatter, to pass
Note : Don't drop the ball near or onto a vent hole /rivet hole  
 
4. SCRATCH TEST (PRESSURE TEST)
Use 120-grit (abrasive paper ) sandpaper to scratch two side and three directions 15 times, then put into room temperature water for 15 minutes, it pass if no breakage and no crack.
 
5. POLOLARISCOPE CHECK
To test the balance of compressive stress and tensile stress depends on the color what you see.
 
6. FRAGMENTATION CHECK
Apply tape (adhesive film)on the convex (front) surface of the lid, domed side upward, break it with a hammer broken 5X5cm measuring range , number of particles (fragments) counted should be at least 40,
The purpose of this test is to determine whether the glass has been adequately toughened.