China Y2o3 Zro2 Zirconium Oxide Ceramic Zirconia Crucible for Melting, Find details about China Zirconia Grinding Jar, Ceramic Grinding Jar from Y2o3 Zro2 Zirconium Oxide Ceramic Zirconia Crucible for Melting
Type 1: Cylindrical ceramic crucibles
Model# | Outer diameter(mm) | Height(mm) | Wall thickness(mm) | Volume(ml) |
JT2030 | 20 | 30 | 1.5 | 10 |
JT3030 | 30 | 30 | 1.8 | 15 |
JT3060 | 30 | 60 | 1.8 | 30 |
JT3645 | 36 | 45 | 2.5 | 30 |
JT4032 | 40 | 32 | 1.6 | 30 |
JT4050 | 40 | 50 | 2.5 | 45 |
JT4342 | 43 | 42 | 1.8 | 50 |
JT6060 | 60 | 60 | 2.5 | 130 |
JT5590 | 59 | 90 | 2.5 | 200 |
JT10040 | 100 | 40 | 5.5 | 200 |
JT8080 | 80 | 80 | 3.3 | 350 |
JT100100 | 100 | 100 | 4.0 | 550 |
JT135160 | 135 | 160 | 6.0 | 2000 |
Model# | Upper OD(mm | Bottom OD (mm) | Height(mm) | Wall thickness (mm) | Volume (ml) |
JT2020-14 | 25 | 14 | 20 | 1.5 | 5 |
JT3030-18 | 30 | 18 | 30 | 1.7 | 10 |
JT3438-20 | 34 | 20 | 38 | 1.9 | 20 |
JT4640-25 | 46 | 25 | 40 | 2 | 30 |
JT5645-30 | 56 | 30 | 45 | 2.9 | 50 |
JT5553-48 | 55 | 48 | 53 | 2.5 | 90 |
JT5768-37 | 47 | 37 | 68 | 3.5 | 100 |
JT5572-48 | 55 | 48 | 72 | 2.6 | 140 |
JT-7085-44 | 70 | 44 | 85 | 2.9 | 200 |
JT7590-50 | 75 | 50 | 90 | 2.9 | 300 |
JT80110-65 | 80 | 65 | 110 | 3.3 | 400 |
JT 100120-70 | 100 | 70 | 120 | 3.5 | 600 |
JT105150-70 | 105 | 70 | 150 | 4.5 | 800 |
JT113160-75 | 113 | 75 | 160 | 3.5 | 1200 |
JT125155-80 | 125 | 80 | 155 | 3.5 | 1200 |
Model# | Shape | Length(mm) | Width(mm) | Height(mm) | Wall thickness(mm) | Volume(ml) |
JT272310 | Rectangular | 27 | 23 | 10 | 2 | 5 |
JT971712 | Rectangular | 97 | 17 | 12 | 2 | 7 |
JT603015 | Rectangular | 60 | 30 | 15 | 2 | 20 |
JT1002020 | Rectangular | 100 | 20 | 20 | 2 | 25 |
JT757540 | Square | 75 | 75 | 40 | 2.5 | 130 |
JT858540 | Square | 85 | 85 | 40 | 3 | 200 |
JT15512055 | Rectangular | 155 | 120 | 55 | 5.5 | 550 |
JT10010040 | Square | 100 | 100 | 40 | 4 | 550 |
JT16016078 | Square | 160 | 160 | 78 | 6 .5 | 1400 |
Property | Units | Materials | ||||
99.5%Al2O3 | 99%Al2O3 | 95%Al2O3 | ZrO2 | Si3N4 | ||
Density | g/cm3 | ≥3.85 | ≥3.80 | ≥3.60 | ≥6.0 | ≥3.2 |
Water absorption | % | 0 | 0 | 0 | 0 | 0 |
Hardness | HV | 1700 | 1700 | 1500 | 1300 | 1550 |
Flexural strength | Mpa | ≥379 | ≥338 | ≥320 | ≥1200 | ≥600 |
Compressive strength | Mpa | ≥2240 | ≥2240 | ≥2000 | ≥1990 | ≥2500 |
Fracture toughness | Mpa m1/2 | 4-5 | 4-5 | 3-4 | 6.5-8 | 6 |
Max. service temperature (Non-loading) | ºC | 1675 | 1600 | 1500 | 1000 | 1200 |
CTE (20-800ºC) | 1×10 -6 /ºC | 6.5~8.0 | 6.2~8.0 | 5.0~8.0 | 8.0~9.5 | 3.1 |
Thermal shock | T(ºC) | ≥250 | ≥200 | ≥220 | ≥300 | ≤1000 |
Thermal conductivity(25ºC) | W/m.k | 30 | 29 | 24 | 3 | 15~20 |
Volume resistivity (25ºC ) | ohm.cm | >1 x 10 14 | >1 x 10 14 | >1 x 10 14 | >1 x 10 11 | >1 x 10 12 |
Insulation strength | KV/mm | 19 | 18 | 18 | 17 | |
Dielectric constant(1Mhz) | (E) | 9.7 | 9.5 | 9.5 | 29 |