Material | laminas de PVC | PU sandwich panel | PPGI steel roof | Aluminium | Fiber cement |
Color stable | 20-25 years | 5-8 years | 5-8 years | 15 years | 10 years |
Warranty | 20 years | 15 years | 10 years | 15 years | 10 years |
Anti-rust | Good | Bad | Bad | Good | Good |
Thermal conductivity | Good: 0.13 W/(m·K) | Good: 0.09 W/(m·K) | Bad: 15 W/(m·K) | Bad: 20 W/(m·K) | Good: 0.11 W/(m·K) |
Impact resist | Good | Good | Good | Good | Bad |
Soundproof | Excellent | Excellent | Bad | Bad | Excellent |
Thickness | 2.0mm | 35mm | 0.5mm | 1mm | 6mm |
Weight | 3.9kg/m2 | 12kg/m2 | 5kg/m2 | 5kg/m2 | 12kg/m2 |
Quantity/40HQ | 7000m2 | 1000m2 | 5000m2 | 5000m2 | 2400m2 |
Price | Middle | Higher | Middle | Higher | Lower |
3 Layers Corrugated laminas de PVC Project Show
Insulation 3 Layers laminas de PVC Technical Data
Heat-Resistance | (72°c,6h)no deformatio, no viscousness | High-low temperature change | ±0.11% |
Cold-Resistance | (-40 °c,6h) no crack in suirface | Fire-protection | Class B1 Retardant Building Materials |
Bending capability | 25mm | Vicat softening temperature | ≥75°c |
Flexural load | 800N, no crack | Water absorption rate | ≤0.05% |
Fleural strength | 72MPa | Nail force | ≥46N |
Tensile strength | 30MPa | Chemical resistance properties | No reaction |