Low P Welding Grade Bauxite Chinese Bauxite, Find details about China Bauxite, Welding from Low P Welding Grade Bauxite Chinese Bauxite
Main specification of Welding Grade Bauxite: | |||||
Al2O3 (min.) | 87.00% | 86.00% | 85.00% | 84.00% | 83.00% |
Fe2O3 (max.) | 2.00% | 2.00% | 2.20% | 2.30% | 2.50% |
TiO2 (max.) | 4.50% | 4.50% | 5.00% | 5.00% | 5.00% |
K2O+Na2O (max.) | 1.00% | 1.00% | 1.00% | 1.00% | 1.00% |
CaO+MgO (max.) | 0.70% | 0.70% | 0.70% | 0.70% | 0.70% |
P (max.) | 0.04% | 0.04% | 0.04% | 0.04% | 0.04% |
S (max.) | 0.02% | 0.02% | 0.02% | 0.02% | 0.02% |