Item | Test method | Test data | Data unit |
Density | 0.963-0.967 | g/cm3 | |
MFR(190ºC,2.16KG) | 5.80 | g/10min | |
Tensile yield strength | 200 | Kg/cm2 | |
Powder ash | 0.04 | wt% | |
Elongation at break | 500 | % |
Item | Test method | Test data | Data unit |
Density | GB/T1033- 1986 | 0.956 | g/cm3 |
MFR(190ºC,2.16KG) | GB/T3682- 2000 | 2.2 | g/10min |
Tensile yield strength | GB/T1410/ 1992 | 24.0 | Mpa |
Elongation at break | GB/T1410/ 1992 | 600 | % |
IZOD Impact Strength | GB/T1413/ 1993 | 13 | Kg/m2 |
Flexural modulus | GB/T1843- 1996 | 1000 | Mpa |
Item | Test method | Test data | Data unit |
Density | 0.963 | g/cm3 | |
MFR | 8.2 | g/10min | |
Tensile yield strength | ≥10.0 | Mpa | |
Tensile breaking strength | ≥30.0 | Mpa | |
Elongation at break | ≥140 | % |
Item | Test method | Test data | Data unit | |
Density | GB/T 1033 | 0.948 | g/cm3 | |
MFR | 190ºC/5.0kg | GB/T 3682 | 0.25 | g/10min |
190ºC/21.6kg | GB/T 3682 | 6.4 | ||
Tensile yield strength | GB/T 1040 | ≥23 | Mpa | |
Volatile component | GB/T156581 | ≤ 350 | Mg/kg | |
Elongation at break | GB/T 1040 | ≥600 | % | |
CHARPY Impact Strength | GB/T 1043 | ≥25 | KJ/m2 | |
Cleanliness(colored particle) | SH/T 1541 | ≤ 20 | Per/kg | |
Cleanliness(impurities) | SH/T 1541 | ≤ 60 | Per/kg |
Performance | Test Method | Test data | Data unit |
Melt flow rate | Q/SY DS 0511 | 20 | g/10min |
Density | Q/SY DS 0510 | 956.4 | g/cm3 |
tensile yield stress | Q/SY DS 0512 | 28.6 | Mpa |
tensile breaking stress | Q/SY DS 0512 | 5.7 | Mpa |
tensile breaking strength | Q/SY DS 0512 | 115 | % |