Name | Technique | Material | Dia/mm | Wall thickness | Length/mm |
Forging shaft | Forging+turning+grinding | alloy steel carbon steel stainless steel | 200-800 | ---- | 500-20000 |
Hollow shaft | Forging+drilling+turning | 150-800 | ≥15mm | ≤17000 | |
Shaft sleeve | Forge+drill & bore+turning +milling | 400-700 | ≥15mm | ≤18000 | |
Large bolt | Rolled/forge+turning+threading | 300-800 | ---- | ≤17000 | |
Hydraulic cylinder | Forging+drill & bore+ turning | 300-2000 | ≥10mm | ≤10000 | |
Other parts in deep-hole | Forge+ drill & bore+turning+mill | 300-2000 | ---- | ≤20000 |
Item | Process | Facility | Inspection items | Standard |
01 | Steel material inspection | Chemical composition (EF+LF+VD) | Material standard | |
surface | Ingot inspection specification | |||
Ingot type and weight | Material standard | |||
02 | Material store | Division put | warehouse management | |
1 | Heat | Heat furnace | Temperature/Time | Heating process specification Forging production procedure |
2 ↓ | Forging | Press | Reduction ratio,forging temperature,deformation, Surface and dimensions | Forging process card Forging procedure |
3 ↓ | Heat treatment | heat treatment furnace | heat treatment charts | 1st heat-treatment card Forging procedure |
4 ↓ | Rough inspection | Dimensions, apperance, Mark | Inspection specification Forging procedure | |
5 ↓ | Rough UT | UT equipment | Single defect, concentrated Defects bottom wave attenuation | UT standard or customer's technical requirements |
6 ↓ | Saw cutting | Saw machine | Dimension | IQC and forging |
7 ↓ | rough turning | turning-lathe | Dimension,appearance | Rough machining drawing |
8 ↓ | UT | UT equipment | Single defect, concentrated defects bottom wave attenuation | UT standard or customer's technical requirements |
9 ↓ | Q+T heat treatment | heat treatment furnace | heat treatment charts | Heating process specification |
10 ↓ | Sampling or machining | machining tool | rough machining drawing sampling drawing | sample machining drawing |
11 ↓ | mechanical property test | tensile testing machine/ impact testing machine | ambient temperature,humidity, Test temp.Sample dimension, test method | Standard technical specification |
12 ↓ | finish machining | machining tool | Dimension,appearance | finish machining drawing |
13 ↓ | UT | UT equipment | Single defect, concentrated Defects bottom wave attenuation | UT standard or customer's technical requirements |
14 ↓ | MT | MT equipment | Magnetic particle indication | Test standard or Technical requirements |
15 ↓ | Mark | Steel seal | marking content | Product standard Technical requirements Forging process |
16 ↓ | Final inspection | Appearance, dimension, mark acceptance inspection | Product inspection specification Product standard P.O. | |