Welding can be accomplished by the gas-shielded processes using a tungsten electrode or a consumable electrode. Postweld heat treatment of the weld are not necessary to maintain corrosion resistance. Heavy restrained sections can be welded and the weld's mechanical properties follow the same trends as base metal properties. Standard practices such as clean surfaces, good joint alignment, U-joints for thicker sections, etc., should be followed.
Standards: ASME SB-444; ASME SB-829; ASME SB-751; ASME SB-704
AMS 5581
Density: 8.44G/cm3
Size: O. D. Φ 1m~220mm; WT: 0.1mm~10mm
Monthly export quantities: 20tons
Exported country: Italy, United Kingdom, Germany, Netherlands, Canada, Spain, Argentina
Chemical Analysis of ALLOY 625 |
C | MN | P | S | Si | Cr | Ni | Mo | Co | Ti | Al | Fe | Nb |
0.10 | 0.50 max | 0.015max | 0.015 max | 0.50max | 20.0 -23.0 | 58.0 min | 8.0 - 10.0 | 1.0 max | 0.40 max | 0.40 max | 5.0 max | 3.15 - 4.15 |
Mechanical Properities(Under Room Temperature) |
Yield Strength,min,(Mpa) | Tensile Strength,min,(Mpa) | Elongation,min,(%) |
276 | 690 | 30 |