1j79 Soft magnetic alloy tube E11c Permalloy tube malloy tube

China 1j79 Soft magnetic alloy tube E11c Permalloy tube malloy tube, Find details about China 1j79, Permalloy tube from 1j79 Soft magnetic alloy tube E11c Permalloy tube malloy tube

Model NO.
E11C
density
8.6
Curie point
450
Saturation magnetostriction coefficient
2.0
Trademark
Permalloy
Transport Package
Inner Core, Waterproof Paper, Wooden Case
Origin
China
HS Code
722699900
Model NO.
E11C
density
8.6
Curie point
450
Saturation magnetostriction coefficient
2.0
Trademark
Permalloy
Transport Package
Inner Core, Waterproof Paper, Wooden Case
Origin
China
HS Code
722699900
1J79/ Permalloy tube/ E11c tube 79HM alloy

Classification: precision soft magnetic alloy
Supplement: Alloy with high permeability in weak fields at saturation induction 0.65-0.75 T. Alloy 1J79/ permally high squareness of the hysteresis loop and a low coefficient of magnetization reversal
Application: For small cores of transformers, chokes and relays operating in weak fields, magnetic shields. In the small thickness (0.05 ± 0.02 mm) - cores for pulse transformers, magnetic amplifiers and solid state relays
Chemical Composition,%:

 

 Ni 
78.5 - 80% 

Fe 
13.73 - 16.8% 


0.03% 

Si 
0.3 - 0.5% 

Mn 
0.6 - 1.1% 


o 0.02% 


0.02% 

Mo 
3.8 - 4.1% 

Ti 
0.15% 

Al 
0.15% 

Cu 
0.2%
 

Basic physical constants and mechanical properties of the alloy:
Density: γ = 8,6 g / cm3;
Electric resistivity: ρ = 0,55 ohm mm2 ? / m;
The temperature of the Curie point: Θs = 430 ° C;
Saturation magnetostriction: λS = 2 ? 106;
Brinell hardness of 210/120 HB;
Ultimate: RM = 1030/490 MPa;
Yield strength: σ0,2 = 980 145 MPa;
Modulus of elasticity E = 210 kN / mm2;
Elongation: δ5 = 3/50%;
Relative compression: φ = -%.

Heat treatment of the alloy
AnnealingTemperature and heating rateHolding time, hCooling mode
Vacuum with a residual pressure not higher than 10-3 Torr. Art. or pure hydrogen with a dew point of not higher than minus 40 ° C.(1125 ± 25) ° C not higher than 500 ° C / h3-6to 600 ° C at a rate not exceeding 200 ° C / h from 600 to 200 ° C at a rate of at least 400 ° C / h
 
The magnetic properties of the alloy
 
TypeClassThickness or diameter, mmInitial permeabilityMax. permittivityCoercive forceTechnical saturation induction
mH / mG / EmH / mG / EA/mE(10-4 G)
no lessno moreno less

cold-rolled strips



1
0,0058,8700038300008,00,100,75
0,0117,51400075600005,60,07
0,02201600088700004,00,05
0,05
0,08
2016000110900003,20,04
 0,10
0,15
25200001501200002,40,03
Cold rolled sheets and strips0,20
0,25
28220001601300001,60,02
0,35
0,50
0,8
1,0
31250001901500001,60,02
1,5
2,0
2,5
28220001601300001,60,02
cold drawn wire
hot rolled sheets
0,05
0,10
6,3500050400006,40,08
3-222520000100800003,20,04
Bar8-1002520000100800003,20,04
cold-rolled strips20,00512,51000044350006,40,080,73
0,012016000110900003,20,04
0,0225200001251000002,40,03
0,05
0,08
25200001501200001,60,02
0,10
0,15
28220001901500001,20,015
0,20
0,25
3125000230180001,20,015
0,35
0,5
0,8
1,0

38

30000

280

220000

1,0

0,012
1,5; 2,031250002301800001,20,015
cold-rolled strips30,012520000150120002,40,030,73
0,0231250001901500001,60,02
0,0538300002502000001,20,015
0,1038300002502000001,20,015
0,20
0,25
38300002802200001,00,012
0,3544350003102500001,00,012

1j79 Soft magnetic alloy tube E11c Permalloy tube malloy tube
1j79 Soft magnetic alloy tube E11c Permalloy tube malloy tube
1j79 Soft magnetic alloy tube E11c Permalloy tube malloy tube