China 1j79 Permalloy Sheet Permalloy 80, Find details about China 1j79, Permalloy from 1j79 Permalloy Sheet Permalloy 80
Description
Permalloy 80 is an alloy of nickel, iron and molybdenum. It is a soft magnetic alloy with exceptionally high magnetic permeability. The alloy has a low coercivity, near zero magnetostriction, and significant anisotropic magnetoresistance. The low magnetostriction is critical for industrial applications,
where variable stresses in thin films would otherwise cause a ruinously large variation in magnetic properties.
Parameter
TABLE 1 Chemical Requirement
Eelement | C≤ | P≤ | S≤ | Mn | Si | Cu≤ | Mo | Ni | Fe |
Composition% | 0.03 | 0.02 | 0.02 | 0.6-1.1 | 0.3-0.5 | 0.20 | 3.8-4.1 | 78.5-80.0 | Remainder |
Notes:
The shape and dimensions of the alloys are in compliance with GBn198-88
TABLE 2 Physical Requirement
Property | Resisitivity(μΩM) | Desinty(g/cm3) | Curie Point.C | High saturation magneto-striction coeffientλθ/10-6 |
Value | 0.55 | 8.6 | 450 | 2 |
TABLE 3 AC Magnetic Properties for Strip(min Value)
Thickness | The peak for the magnetic field strength is 0.1A/m,Under different frequencise of flexible magnetic permeability μm/(mH/m) | |||
60Hz | 400Hz | 1KHz | 10KHz | |
0.02 | 17.5 | 12.5 | ||
0.05 | 18.8 | 9.4 | ||
0.10 | 22.5 | 15 | ||
0.20 | 12.5 | 7.5 | ||
0.35 | 25 | 8.8 |
TABLE 4 Coefficient of Linear Expansion at different Temperature/(x10-6)
Temp | 20-100°C | 20-200ºC | 20-300ºC | 20-400ºC | 20-500ºC | 20-600ºC | 20-700ºC |
Value | 1.3-10.8 | 10.9-11.2 | 14.4-12.9 | 11.9-12.5 | 12.3-13.2 | 12.7-13.4 | 13.1-13.6 |
TABLE 5 Magnetic Requirement (Cold rolling Strip)
Grade I
(δ&D)/mm | μ0.08/(mHm)≥ | μm(mHm)≥ | Bs/T≥ | Hc(A/M)≤ |
0.005 | 12.5 | 44.0 | 0.75 | 6.4 |
0.01 | 17.5 | 87.5 | 0.75 | 4.8 |
0.02-0.04 | 20.0 | 112.5 | 0.75 | 4.0 |
0.05-0.09 | 22.5 | 137.5 | 0.75 | 2.8 |
0.10-0.19 | 25.0 | 162.5 | 0.75 | 2.0 |
0.20-0.34 | 28.0 | 225.0 | 0.75 | 1.6 |
0.35-1.00 | 30.0 | 250.0 | 0.75 | 1.2 |
1.10-2.50 | 27.5 | 225.0 | 0.75 | 1.6 |
2.50-3.00 | 26.3 | 187.5 | 0.75 | 2.0 |
Grade II
(δ&D)/mm | μ0.08/(mHm)≥ | μm(mHm)≥ | Bs/T≥ | Hc(A/M)≤ |
0.02-0.04 | 22.5 | 125.0 | 0.75 | 2.4 |
0.05-0.09 | 25.0 | 150.0 | 0.75 | 2.0 |
0.10-0.19 | 27.5 | 187.5 | 0.75 | 1.6 |
0.20-0.34 | 31.3 | 250.0 | 0.75 | 1.2 |
0.35 | 32.5 | 275.0 | 0.75 | 0.79 |
Grade III
(δ&D)/mm | μ0.08/(mHm)≥ | μm(mHm)≥ | Bs/T≥ | Hc(A/M)≤ |
0.01 | 25.0 | 150.0 | 0.73 | 2.4 |
0.02-0.04 | 31.0 | 190.0 | 0.73 | 1.6 |
0.05-0.09 | 38.0 | 250.0 | 0.73 | 1.2 |
0.10-0.19 | 38.0 | 250.0 | 0.73 | 1.2 |
0.20-0.34 | 38.0 | 280.0 | 0.73 | 1.0 |
0.35 | 44.0 | 310.0 | 0.73 | 1.0 |
Hot Rolling(forging) Flastspring
(δ&D)/mm | μ0.08/(mHm)≥ | μm(mHm)≥ | Bs/T≥ | Hc(A/M)≤ |
3-22 | 25.0 | 125 | 0.75 | 2.4 |
Hot Rolling (Forging)Bar
(δ&D)/mm | μ0.08/(mHm)≥ | μm(mHm)≥ | Bs/T≥ | Hc(A/M)≤ |
8-100 | 25.0 | 125.0 | 0.75 | 2.4 |