Incoloy 825 is a Nickel-Iron-Chromium alloy with additions of Molybdenum and Copper. It has excellent resistance to both reducing and oxidising acids, to stress-corrosion cracking and to localised pitting and crevice corrosion. It is also especially resistant to sulphuric and phosphoric acids.
Chemical CompositionSpecificationsDesignationsKey FeaturesTypical Applications
ElementMin %Max %
Ni38.0046.00
Co-2.00
Cu1.503.00
Cr19.5023.50
Mo2.503.50
Al-0.20
C-0.05
Si-0.50
Mn-1.00
S-0.03
Ti0.601.20
FeBal
ASTM B425
BS 3075 NA 16
BS 3076 NA 16
ISO 15156-3
(NACE MR 0175)
W.Nr 2.4858
UNS N08825
AWS 022
Resistant to reducing environments such as those containing sulphuric and phosphoric acids
Resistant to a variety of oxidising substances such as nitric acid and nitrates
Resistant to chloride-ion stress corrosion cracking and, pitting & crevice corrosion
Good for chemical processing
Chemical Processing
Nuclear Fuel Reprocessing
Acid Production
Pickling Equipment
Density8.14 g/cm³0.294 lb/in³
Melting Point1400°C2550°F
Coefficient of Expansion14.0 μm/m °C (20 - 100°C)7.8 x 10-6 in/in °F (70 - 212°F)
Modulus of Rigidity75.9 kN/mm²11009 ksi
Modulus of Elasticity196 kN/mm²28428 ksi
Heat Treatment of Finished Parts
Condition as supplied by Alloy WireTypeTemperatureTime (Hr)Cooling
°C°F
Annealed or Spring TemperStress Relieve450 - 470840 - 8800.5 - 1Air
Properties
ConditionApprox. tensile strengthApprox. operating temperature
N/mm²ksi°C°F
Annealed600 - 80087 - 116-100 to +250-145 to +480
Spring Temper800 - 1100116 - 159-100 to +250-145 to +480

The above tensile strength ranges are typical. If you require different please ask.