China Super Molybdenum Disilicide (MoSi2) Heating Element in High Temperature Furnace, Find details about China Mosi2 Heating Element, Mosi2 Heater from Super Molybdenum Disilicide (MoSi2) Heating Element in High Temperature Furnace
2. Physics Characters: | |||||
Volume Density | Bending Strength | Vickers Hardness | Porosity | Water absorption | Heating Elongation Rate |
5.5g/cm3 | 15-25 kg/cm3 | (HV)570kg/mm2 | 7.40% | 1.20% | 4% |
Atmosphere | The Maximum Using Temperature of Elements | |
1700 | 1800 | |
No2 ,Co2 ,O2 ,Air | 1700°C | 1800°C |
He ,Ar ,Ne | 1650°C | 1750°C |
SO2 | 1600°C | 1700°C |
CO ,H2 | 1500°C | 1600°C |
Dry H2 | 1350°C | 1450°C |