Graphite Crucibles for Melting Gold Silver

China Graphite Crucibles for Melting Gold Silver, Find details about China Graphite Crucible, Crucible from Graphite Crucibles for Melting Gold Silver

Transport Package
Wooden Packing Box
Origin
Zibo, Shandong
HS Code
6903900000
Transport Package
Wooden Packing Box
Origin
Zibo, Shandong
HS Code
6903900000
Graphite Crucibles for Melting Gold SilverGraphite Crucibles for Melting Gold SilverGraphite Crucibles for Melting Gold SilverGraphite Crucibles for Melting Gold Silver
Advanced technology
Crucibles are manufactured by the worlds most advanced cold isostaticmolding method, with isotropic properties, high density high strength, denseuniform and defect-free
Great variety of goods
Produce resin bond and clay bond crucible, Provide the best solution fordifferent customers, to extend the service life
Long life
Crucible life is 2-5 times longer than ordinay
Resistance to chemical attack
Advanced materials and glaze recipes, effectively resistance to chemicalerosion
Graphite Crucibles for Melting Gold Silver
High thermal conductivity
Usingnatural graphite materials and isostatic pressing, thin crucible wallfast heat conduction
Resistance to hightemperature
Crucible temperature range 400-1400ºC 
Energy-saving
Crucible made of high thermal conductivity material can bring a largenumber of energy savings for users in the production process.
Less pollution
Because of the choice of high purity inorganic material, little or no harmfulimpurities into products in the metal melting process
Good oxidation resistance
The appearance of a crucible has multi-special glaze layers, ciupled withthe molding material compact, greatly improving the corrosion resistance ofthe product, and extending the life of the crucible
Stable and reliable quality
Part of the main raw materials of foreign well-known brands used glazesmainly using imported raw materials. The quality is stable and reliable
PREHEATING PROCEDURE OF CRUCIBLE USED FOR THE FIRST TIME
1. After the crucible is put into the furnace, the crucible is heated slowly, and the temperature reaches 200 ºCC after two hours to remove the warm gas in the crucible
2. Then the crucible was heated to 600 ºC after 15 hours with low power, and then the temperature was 950 ºC after half an hour with full heating power, holding for about 1.hour. In this way, the glaze layer can be fully melted, the oxidation resistance can be mproved, and the maximum service life of the crucible can be ensured
3. Heat preservation for 1 hour before feeding as required
4. The curve is shown in the green line

THE PREHEATING PROCEDURE FOR REUSING THE CRUCIBLE IS AS FOLLOWS 
1. Firstly, the crucible is heated slowly, and the temperature reaches 600 ºC aftertwo hours to remove the moisture in the crucible. At the same time, the glaze layer and anti-oxidation coating on the surface of the crucible are fully sintered to prevent oxidation and prolong the service life of the crucible 
2. Then continue heating, and make the temperature reach 950 ºC after half an hour, holding for about 1 hour. 
3. Heat preservation for 1 hour before feeding as required 
4. The curve is shown in the red line Graphite Crucibles for Melting Gold SilverGraphite Crucibles for Melting Gold SilverGraphite Crucibles for Melting Gold SilverGraphite Crucibles for Melting Gold Silver
Our Advantages

The crucibles produced by our company are suitable for melting aluminum, copper, gold, silver and other non-ferrous metals, and are exported to many foreign countries and have gained a good reputation.


About packaging:
The products in the wooden packing box are packed in PE moisture-proof bags. Or can be customized according to your requirements

Our strengths:
1,Long life :Crucible life is 2-5 times longer than ordinay
2,Resistance to chemical attack :Advanced materials and glaze recipes,effectively resistance to chemical erosion 
3,High thermal conductivity Usingnatural grephite materials and isostatic pressing,thin crucible wall, fast heat conduction
4,Resistance to high temperature: Crucible temperature range 400-2000ºC
5,Energy-saving :Crucible made of high thermal conductivity material can bring a large number of energy savings for users in the production process.
6,Less pollution :Because of the choice of high purity inorganic material ,little or no harmful impurities into products in the metal melting process
7,Good oxidation resistance :The appearance of a crucible has multi-special glaze layers ,ciupled with the molding material compact ,greatly improving the corrosion resistance of the product, and extending the life of the crucibleGraphite Crucibles for Melting Gold SilverGraphite Crucibles for Melting Gold SilverTHE COMMON PROBLEM an ALYSIS 
Slow heat conduction 
Not preheating according to the standard procedure 
Slag influences heat conduction 
The crucible has reached its service 

Crucible corrosion 
Adding flux before metal is molten or excessive use of flux 
Certain fluxes contain corrosion substances 
Fuel containing corrosive substances 
Abnormal high-temperature operation may result in glaze layer smelting resembling corrosion 

Top problems 
Repeatadly top impacted on top area cause oxidation 
Slage accumulated arround the top area or between the top area and the furnace cover 
Small gape between the top and the furnace coverlow temperature on top area 
Contacting with some matels with lager heat exchanging coefficients 
Excentral installation cause not enough space between the top and fueace 

Excessive oxidation
Flame in furnace against the bottom of the crucible directLow temperature in the top area
Overheated working temperatureHoisting or moving improperly damagesglaze lager
The emergent drain hole is open 

Exliosion 
Heating rapidly while the crucible has damped during transportation or storage 
Over rapid heating-up during preheating procedure 
The added materials are not completely dried 

Middle or bottom craks 
Lmpacted during transportation or installation 
Crucible should be placed in the middle of the furnace stack smoothly and stably 
An improper graphite stand is uesd 
The existence of great thermal difference in the furnace 
Matel ingots in the crucible filled horizontally or diagonally 
Metal materials overfilled 
Leftover slag or molten matal in the crucible 

 

FAQ

1. How can I get your prompt quotation?

A: we can give you reply with quotation quickly if you kindly send the inquiry with following factors:
 top diameter, bottom diameter, thickness, height, application and quantity. 

2.What's the MOQ of the order?
No limit, we can offer the best suggestions and solutions according to your condition.

3. How to solve the quality problems?
If the products don't conform to customer's samples or have quality problems, our company will be responsible for it.

4. How to solve the packaging?
We use wooden box packaging

5. Product delivery cycle?
the product production cycle is 12 days, the specific production quantity and cycle look forward to your negotiation

6. What are the transportation logistics?
by sea, by air, by courier, by post, etc.

7. Can it be customized?
We accept customization.

8.We have professional designers.

9.We have a professional after-sales department to answer your questions.