China High Temperature Fluids Resistance Diesel Resistant Elastomeric Tubing Heat Shrink, Find details about China Diesel Resistant Elastomeric Tubing Heat Shrink, Diesel Resistant Tubing Heat Shrink from High Temperature Fluids Resistance Diesel Resistant Elastomeric Tubing Heat Shrink
Item | Test method | Typical data | |
Tensile strength (Mpa) | Before aging | ASTM D638 | ≥12 |
After aging | ISO 188 (166ºC/168h) | ≥8 | |
Elongation (%) | Before aging | ASTM D638 | ≥400 |
After aging | ISO 188 (166ºC/168h) | ≥220 | |
Fluid resistance strength(Mpa) | ISO 37 24hrs. (diesel 70ºC,hydraulic 70ºC, lubricant 100ºC) | ≥8 | |
Fluid resistance elongation (%) | ISO 37 24hrs. (diesel 70ºC,hydraulic 70ºC, lubricant 100ºC) | ≥300 | |
Shrink ratio in axial direction (%) | UL224 | ±10 | |
Heat shock | 4hrs/215ºC | No crack and dripping | |
Flammability | UL224,VW-1 | pass | |
Dielectric strength(KV/mm) | UL224,VW-1 | ≥15 |
Size | As supplied | After recovery | ||
Inch | mm | I.D. MIN (mm) | I.D. MAX (mm) | Wall thickness (mm) |
1/8 | 3.2 | 3.2 | 1.6 | 0.76±0.15 |
3/16 | 4.8 | 4.8 | 2.4 | 0.84±0.15 |
1/4 | 6.4 | 6.4 | 3.2 | 0.89±0.15 |
3/8 | 9.5 | 9.5 | 4.8 | 1.02±0.20 |
1/2 | 12.7 | 12.7 | 6.4 | 1.22±0.20 |
3/4 | 19.0 | 19.0 | 9.5 | 1.45±0.28 |
1 | 25.4 | 25.4 | 12.7 | 1.78±0.28 |
1-1/2 | 38 | 38 | 19.0 | 2.41±0.41 |
2 | 51 | 51 | 25.4 | 2.79±0.41 |
3 | 76 | 76 | 38.0 | 3.18±0.50 |