China Polishing Resin MB300, Find details about China Mixed Bed Resin, Water Softener from Polishing Resin MB300
Items | Units | OH - Form | H + Form | |
Polymer Matrix Structure | --- | Gel PolyStyrene Crosslinked with DVB | ||
Functional Group | --- | Quaternary Amine | Sulfonic acid | |
Volume ratio | --- | 50% | 50% | |
Total Exchange Capacity, min. | eq/l | 1.0 | 1.8 | |
Water Retention Capacity | % | 53-60 | 45-50 | |
Particle Size Distribution | mm | 0.40-1.25 | ||
>1.25 mm max. | % | 5 | 5 | |
<0.40 mm, max | % | 2 | 2 | |
Whole Bead Count, min. | % | 95 | 95 | |
Moisture Content as shipped, max | % | 65 | ||
PH Range, Stability | --- | 0-14 | ||
Shipping weight (approx.) | g/l | 730 | ||
Operating temperature | --- | |||
Ionic conversion, min. | 100°C (212°F) max. | |||
regenerative bed | 60°C (140°F) max. | |||
Ionic conversion, min. | % | 90 | 95 |