China CPP Film Metalized CPP Film CPP Printing Film CPP Bag Made Film VMCPP Film CPP Flower Film, Find details about China VMCPP Film, Mcpp Film from CPP Film Metalized CPP Film CPP Printing Film CPP Bag Made Film VMCPP Film CPP Flower Film
Properties | Test Method | Unit | Typical value | |||
Thickness | Kincess | µm | 20 | 25 | 30 | |
Thickness Variation | ASTM-252-78 | % | ± 3. 0 | ± 3. 0 | ± 3. 0 | |
Tensile strength | MD | ASTM D-882 | MPa | 58 | 56 | 53 |
TD | ASTM D-882 | MPa | 34 | 33 | 32 | |
Elongation At Break | MD | ASTM D-882 | % | 550 | 580 | 590 |
TD | ASTM D-882 | % | 670 | 680 | 690 | |
Friction Coefficient | T/T-US | ASTM D-1894 | - | 0. 68 | 0. 65 | 0. 6 |
T/O-US | ASTM D-1894 | - | 0. 68 | 0. 65 | 0. 6 | |
Heat Shrinkage | MD | ASTM D-1204 | % | 0. 8 | 0. 8 | 0. 8 |
TD | ASTM D-1204 | % | 0. 8 | 0. 8 | 0. 8 | |
Wetting Tension | ASTM D-2578 | Dyn | 38 | 38 | 38 | |
Heat seal temperature | ISO-17557 | ºC | 130 | 128 | 128 | |
Heat seal strength | ISO-17557 | N/15mm | 8 | 8 | 8 | |
Oxygen permeability | ASTM D-3985 | Cm3/m2·d | 38 | 30 | 28 | |
Moisture permeability | ASTM E-96 | g/m2.24h | 0. 9 | 0. 9 | 0. 8 |