95%/99%/99.7% Al2O3 Ceramic Material Parameters | ||||
Item | Test Condition | 95% Al2O3 Ceramic | 99% Al2O3 Ceramic | 99.7% Al2O3 Ceramic |
Bulk Density (g/cm³) | >3.6 | 3.89 | 3.96 | |
Maximum Use Temp(ºC) | 1450 | 1600 | 1650 | |
Water Absorption(%) | 0 | 0 | 0 | |
ROHS Hardness | ≥85 | ≥89 | ≥89 | |
Flexural Strength MPa(psi×10³) | 20ºC | 358(52) | 550 | 550 |
Compressive Strength MPa(psi×10³) | 20ºC | 2068(300) | 2600(377) | 2600(377) |
Fracture Toughness Mpa m½ | K(l c) | 4-5 | 5.6 | 6 |
Thermal Expansion Coefficient(1×10-6/ºC) | 25-1000ºC | 7.6 | 7.9 | 8.2 |
Thermal Conductivity Coefficient(W/m°K) | 20ºC | 16 | 30.0 | 30.4 |
Thermal Shock Resistance(ºC) | △Tc | 250 | 200 | 200 |
Dielectricity Constant | 1MHz.25ºC | 9 | 9.7 | 9.7 |
Dielectric Strength (ac-kV/mm)(ac V/mil) | 8.3(210) | 8.7(220) | 8.7(220) | |
Volume Resistivity (ohm-cm) | 100ºC | >1013 | >1014 | >1014 |
Code | Rim Length (mm) | Bottom Length (mm) | Rim Breadth (mm) | Bottom Breadth (mm) | Height (mm) |
C-211 | 50 | 42 | 28 | 20 | 10 |
C-212 | 50 | 42 | 28 | 20 | 15 |
C-213 | 60 | 52 | 30 | 22 | 15 |
C-214 | 75 | 65 | 35 | 25 | 15 |
C-215 | 90 | 80 | 60 | 50 | 18 |
C-216 | 90 | 80 | 65 | 55 | 18 |
C-217 | 120 | 110 | 60 | 50 | 18 |
C-218 | 120 | 110 | 65 | 55 | 18 |