Ceramic Honeycomb Heater Honeycomb Ceramic Gas Refractory Heater

China Ceramic Honeycomb Heater Honeycomb Ceramic Gas Refractory Heater, Find details about China Ceramic Honeycomb, Cordierite Honeycomb from Ceramic Honeycomb Heater Honeycomb Ceramic Gas Refractory Heater

Model NO.
HCH
Chemical Composition (%)
Al2O3, Sio2, MGO, Fe2o3+TiO2 and Others
Principle
Regenerative Heat Exchanger
Structure Material
Ceramic
Application
Heater
Ceramic Heating Equipment Type
Ceramic Heater
Trademark
DXY
Transport Package
Wooden Box/Carton Box with Pallet
Origin
China
HS Code
6909190000
Model NO.
HCH
Chemical Composition (%)
Al2O3, Sio2, MGO, Fe2o3+TiO2 and Others
Principle
Regenerative Heat Exchanger
Structure Material
Ceramic
Application
Heater
Ceramic Heating Equipment Type
Ceramic Heater
Trademark
DXY
Transport Package
Wooden Box/Carton Box with Pallet
Origin
China
HS Code
6909190000
Cordierite/Corundum/Mullite-based Honeycomb Ceramic Heat Accumulation Substance
It's features of corrosion resistances, large specific surface area, small heat
Resistance, good thermal conductivity and excellent thermal-shock resistance, fast heat exchanging and energy saving. It's widely used in many fields.

Ceramic Honeycomb Heater Honeycomb Ceramic Gas Refractory Heater
Ceramic Honeycomb Heater Honeycomb Ceramic Gas Refractory Heater

The honeycomb ceramic as the heat exchange media is the key part for heat storing HTAC
( High Temperature Air Combustion) technology. It is the best choice for RTO, heat exchanger
And other environmental protection and energy saving products.

Characterics:
1. Low thermal expansion
2. Large specific heat capacity
3. High specific surface area
4. Low pressure drop
5. Small thermal resistance
6. Good thermal conductivity
7. Good heat-shock resisting ability

Application: Iron and steel, metallurgy, petrochemical, electric power, boiler and Fuel elecric plant, Thermal power plant, theheat power station etc.
 
CompositionValue (%)
Al2O370-80
SiO215-25
MgO0-2
Fe2O2+TiO21-3
Others<5
 
IndexUnitValue
Density g/cm32.3-2.7
Coefficient of heat expansion(X10-6K-1) (20-800celsius degree)≤6
Specific Heat(J/Kg.k) (20~1000celsius degree)1100~1300
Thermal Conductivity(20~1000celsius degree)1.5~2.0
Impact Thermal Resistance(celsius degree/min)≥300
Max.Working Temp.celsius degree1550
Water absorption%15~25