3.2mm High Tensile Prestressing Steel Wire

China 3.2mm High Tensile Prestressing Steel Wire, Find details about China Prestressed Concrete Steel Wire, Prestressing Steel Wire from 3.2mm High Tensile Prestressing Steel Wire

Model NO.
PC Steel Wire
Brand Name
Daqiang
Strandard
Astma 421, BS5896, Jisg3536
Strength
1470, 1570, 1670, 1860
Coil Weight
0.4-3.0 Ton / Coil
Delivery Time
7-15 Days Later
Port of Loading
Xingang, China
Weight Tolerance
5% of Total Amount
Payment
T/T, L/C
Trademark
DaQiang
Transport Package
Export Packing
Specification
GB, ASTM, DIN, BS, JISG
Origin
Tianjin, China (Mainland )
Model NO.
PC Steel Wire
Brand Name
Daqiang
Strandard
Astma 421, BS5896, Jisg3536
Strength
1470, 1570, 1670, 1860
Coil Weight
0.4-3.0 Ton / Coil
Delivery Time
7-15 Days Later
Port of Loading
Xingang, China
Weight Tolerance
5% of Total Amount
Payment
T/T, L/C
Trademark
DaQiang
Transport Package
Export Packing
Specification
GB, ASTM, DIN, BS, JISG
Origin
Tianjin, China (Mainland )
Low relaxation high tensile strength pc wire

1. Strandard: ASTM A421, BS 5896, GB/T5223

2. DIA:3.2,3.4, 3.6, 3.8, 4.0, 4.8, 5.0, 6.0, 6.25, 6.7, 7.0, 8.0, 9.0, 10.0mm

3. Tensile Strength: 1470, 1570, 1670, 1770Mpa

4. Surface: Plain, Ribbed, Spiral, Indented.

5. The relaxation at 1000 hour is 1.0-2.0%

6. Material: SWRH 77B, 82B high carbon steel wire rod.

7. Packing: Baling strip, wrapped in anti-rust plastic paper, PP woven cloth

8. Weight: 0.4~2.0 tons per coil




Description: steel wire for pre-stressed concrete, pre-stressing steel wire, high carbon steel wire for pre-tensioning, high tensile low relaxation steel wire, stress-relieved steel wire

Relaxation on 1000 hours: 2.0% max; Elongation at breakage: 4.0% min
Export Packing: baling strip, inside plastic cover, outside PP packing cloth;
Package Weight: 800kg-1600kg
Application: cement electricity poles, railway sleeper, subway track board, concrete piles, beams, girders, slabs, hollow floor board, double-T board, PHC, PPCP.
The  specifications  and  technical  parameters
Nominal  Dia
  (dn/mm)
ToleranceTensile  Strength
  σ b/MPA  Not  less  than
Yield  Stength 
(σ p0.2/MPA)
Not  less  than 
Elongation  at  max  load 
(Lo=200mm)
δ gt/%
Not  less  than
Bending  Times
Not  less  than 
Bending  Radius 
R/mm
Relaxation  Priperties
The  relaxation  at  1000h 
(initial  load  to  70%  of  nominal  tensile  strength  )  (r%)
  Not  more  than 
4.8± 0.051470
1570
1670
1770
1860
1290
1380
1470
1560
1640
3.54152.0
5.0
6.0± 0.051470
1570
1670
1770
1290
1380
1470
1560
415
6.25
7.020
8.0± 0.061470
1570
1290
1380
420
9.025
 3.2mm High Tensile Prestressing Steel Wire
3.2mm High Tensile Prestressing Steel Wire