China Landfill Lake Fish Pond Textured Smooth Surface HDPE Membrane Liner, Find details about China HDPE Geomembrane, HDPE Liner from Landfill Lake Fish Pond Textured Smooth Surface HDPE Membrane Liner
No. | Properties | Test Method | Test Value | |||||||
1 | Thickness(mm) | ASTM D5199 | 0.50 | 0.75 | 1.00 | 1.25 | 1.50 | 2.00 | 2.50 | 3.00 |
2 | Density (g/cm2) | ASTM D1505 | 0.939 | |||||||
3 | Tensile Propeties | |||||||||
Yield Strength(N/mm) | ASTM D6693 | 7 | 11 | 15 | 18 | 22 | 29 | 37 | 44 | |
Break Strength(N/mm) | 13 | 20 | 27 | 33 | 40 | 53 | 67 | 80 | ||
Yield Elongation % | Type IV | 12 | ||||||||
Break Elongation % | 700 | |||||||||
4 | Tear Resistance/N | ASTM D1004 | 62 | 93 | 125 | 156 | 187 | 249 | 311 | 374 |
5 | Puncture Resistance/N | ASTM D4833 | 160 | 240 | 320 | 400 | 480 | 640 | 800 | 960 |
6 | Stress Crack Tesistance/h | ASTM D5397 | 300 | |||||||
7 | Carbon Black | |||||||||
Carbon Black Content % | ASTM D1603 | 2.0-3.0 | ||||||||
Carbon Black Dispersion | ASTM D5596 | Carbon black dispersion for 10 different views 9 in categoried 1 or 2 and 1 in category | ||||||||
8 | Oxidative Induction Time(OIT) | |||||||||
Standard OIT/min | ASTM D3895 | 100 | ||||||||
High Pressure OIT/min | ASTM D5885 | 400 | ||||||||
9 | Oven Aging at 85°C | |||||||||
Standard OIT-% retained after 90 days | ASTM D3895 | 55 | ||||||||
High pressure OIT-% retained after 90 days | ASTM D5885 | 80 | ||||||||
10 | UV Resistance | |||||||||
Standard OIT retained after 1600 hrs | ASTM D3895 | 50 | ||||||||
High pressure OIT retained after 1600 hrs | ASTM D5885 | 50 | ||||||||
11 | Low tempreture impact brittle property at -70°C | _ | Pass | |||||||
12 | Permeability g·cm/(cm2)·Pa | _ | ≤1.0×10-13 |