China Low Resistance CuNi44 Constantan Strip, Find details about China CuNi 44 Strip, Copper Nickel Alloy Strip from Low Resistance CuNi44 Constantan Strip
CuNi44, also called Constantan, has a very low temperature coefficient, high electrical resistance, high ductility and non-corroding properties. It is suitable for use at temperatures up to 600° C (1110° F). As a very malleable, very ductile alloy, it has a very good resistance to oxidation.
The alloy is non-magnetic. It is suitable for electrical resistors, potentiometers, heating wires, heating cables and mats. Ribbons are used for heating of bimetals. Another field of application is manufacturing of thermocouples because it develops a high electromotive force (EMF) in association with others metals.
Copper nickel alloy series:Constantan CuNi40 (6J40), CuNi1, CuNi2, CuNi6, CuNi8, CuNi10, CuNi14, CuNi19, CuNi23,CuNi30, CuNi34, CuNi44.
Size dimension range:
Wire: 0.1-10mm
Ribbons: 0.05*0.2-2.0*6.0mm
Strip: 0.05*5.0-5.0*250mm
Main grades and properties
Type | Electrical resistivity (20degreeΩ mm²/m) | temperature coefficient of resistance (10^6/degree) | Dens ity g/mm² | Max. temperature (°c) | Melting point (°c) |
CuNi1 | 0.03 | <1000 | 8.9 | / | 1085 |
CuNi2 | 0.05 | <1200 | 8.9 | 200 | 1090 |
CuNi6 | 0.10 | <600 | 8.9 | 220 | 1095 |
CuNi8 | 0.12 | <570 | 8.9 | 250 | 1097 |
CuNi10 | 0.15 | <500 | 8.9 | 250 | 1100 |
CuNi14 | 0.20 | <380 | 8.9 | 300 | 1115 |
CuNi19 | 0.25 | <250 | 8.9 | 300 | 1135 |
CuNi23 | 0.30 | <160 | 8.9 | 300 | 1150 |
CuNi30 | 0.35 | <100 | 8.9 | 350 | 1170 |
CuNi34 | 0.40 | -0 | 8.9 | 350 | 1180 |
CuNi40 | 0.48 | ±40 | 8.9 | 400 | 1280 |
CuNi44 | 0.49 | <-6 | 8.9 | 400 | 1280 |
Mechanical Properties
Max Continuous Service Temp | 400ºC |
Resisivity at 20ºC | 0.49±5%ohm mm2/m |
Density | 8.9 g/cm3 |
Thermal Conductivity | -6(Max) |
Melting Point | 1280ºC |
Tensile Strength,N/mm2 Annealed,Soft | 340~535 Mpa |
Tensile Strength,N/mm3 Cold Rolled | 680~1070 Mpa |
Elongation(anneal) | 25%(Min) |
Elongation(cold rolled) | ≥Min)2%(Min) |
EMF vs Cu, μV/ºC (0~100ºC) | -43 |
Micrographic Structure | austenite |
Magnetic Property | Non |