China FeCr27Al7Mo2 FeCrAl alloy resistance strip, Find details about China resistance strip, Thanthal A1 from FeCr27Al7Mo2 FeCrAl alloy resistance strip
FeCrAl Alloy Grade | Chemical Composition % | |||||||||
C | P | S | Mn | Si | Cr | Ni | Al | Fe | Re | Others |
max(≤) | ||||||||||
1Cr13Al4 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.00 | 12.5-15.0 | ---- | 3.5-4.5 | 0.1 | Bal. |
0Cr15Al5 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.00 | 14.5-15.5 | ---- | 4.5-5.3 | 0.1 | Bal. |
0Cr25Al5 | 0.06 | 0.025 | 0.025 | 0.7 | ≤0.60 | 23.0-26.0 | ≤0.60 | 4.5-6.5 | 0.1 | Bal. |
0Cr23Al5 | 0.06 | 0.025 | 0.025 | 0.7 | ≤0.60 | 20.5-23.5 | ≤0.60 | 4.2-5.3 | 0.1 | Bal. |
0Cr21Al6 | 0.06 | 0.025 | 0.025 | 0.7 | ≤1.00 | 19.0-22.0 | ≤0.60 | 5.0-7.0 | 0.1 | Bal. |
0Cr21Al4 | 0.06 | 0.025 | 0.025 | 0.7 | ≤1.00 | 21.0-23.0 | ≤0.60 | 3.0-5.2 | 0.1 | Bal. |
0Cr21Al6Nb | 0.05 | 0.025 | 0.025 | 0.7 | ≤0.60 | 21.0-23.0 | ≤0.60 | 5.0-7.0 | 0.1 | Bal. |
Thanthal A1 | 0.05 | 0.025 | 0.025 | 0.7 | ≤0.40 | 26.5-27.8 | ≤0.60 | 6.0-7.0 | 0.1 | Bal. |
Propertes/Grade | NiCr 80/20 | NiCr 70/30 | NiCr 60/15 | NiCr 35/20 | NiCr 30/20 | |
Main Chemical Composition(%) | Ni | Bal. | Bal. | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
Cr | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
Fe | ≤ 1.0 | ≤ 1.0 | Bal. | Bal. | Bal. | |
Max Working Temperature(ºC) | 1200 | 1250 | 1150 | 1100 | 1100 | |
Resistivity at 20ºC (μ Ω · m) | 1.09 | 1.18 | 1.12 | 1.04 | 1.04 | |
Density(g/cm3) | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
Thermal Conductivity (KJ/m· h· ºC) | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
Coefficient of Thermal Expansion(α × 10-6/ºC) | 18 | 17 | 17 | 19 | 19 | |
Melting Point(ºC) | 1400 | 1380 | 1390 | 1390 | 1390 | |
Elongation(%) | > 20 | > 20 | > 20 | > 20 | > 20 | |
Micrographic Structure | austenite | austenite | austenite | austenite | austenite | |
Magnetic Property | nonmagnetic | nonmagnetic | nonmagnetic | nonmagnetic | nonmagnetic |