nickel chromium ni80cr20 nikrothal 80 alloy heating element ribbon

China nickel chromium ni80cr20 nikrothal 80 alloy heating element ribbon, Find details about China ni80cr20, nikrothal 80 from nickel chromium ni80cr20 nikrothal 80 alloy heating element ribbon

Model NO.
Ni80Cr20
Origin
Shanghai
Model NO.
Ni80Cr20
Origin
Shanghai
Grade
Cr20Ni80
0.565Thickness
0.56-5mm
Width
6-50mm
Surface
acide washed/bright/oxidized
Weight
25-30kg/roll
Resistivity
1.09±0.05μΩ.m
Highest temperature
1200ºC
Density
8.4g/cm³
Tensile strength
750N/mm²
Elongation
≥20%

Nickel chromium ni80cr20 nikrothal 80 alloy heating element ribbon
 
Grade
Highest temperature
Resistivity
Melting point
Tensile strength
Elongation
0Cr21Al4
1100ºC
1.23±0.06μΩ.m
1500ºC
750
≥12
0Cr25Al5
1250ºC
1.42±0.07μΩ.m
1500ºC
750
≥12
0Cr21Al6Nb
1350ºC
1.43±0.07μΩ.m
1510ºC
750
≥12
0Cr27Al7Mo2
1400ºC
1.53±0.07μΩ.m
1520ºC
750
≥10
KSC
1350ºC
1.44±0.05μΩ.m
1510ºC
750
≥16
Cr20Ni80
1200ºC
1.09±0.05μΩ.m
1400ºC
750
≥20
Cr15Ni60
1150ºC
1.12±0.05μΩ.m
1390ºC
750
≥20
Cr20Ni35
1100ºC
1.04±0.05μΩ.m
1390ºC
750
≥20
Cr20Ni30
1100ºC
1.04±0.05μΩ.m
1390ºC
750
≥20
Grade
    Chemical composition%
C
P
S
Mn
Si
Cr
Ni
Al
Fe
0Cr21Al4
0.12
0.025
0.025
0.7
≤1.0
17-21
≤0.6
3-4
balance
0Cr25Al5
0.06
0.025
0.02
0.5
≤0.6
23-26
≤0.6
4.5-6.5
balance
0Cr21Al6Nb
0.05
0.025
0.02
0.5
≤0.6
21-23
≤0.6
5-7
balance
0Cr27Al7Mo2
0.05
0.025
0.02
0.2
≤0.4
26.5-27.8
≤0.6
6-7
balance
Cr20Ni80
0.08
0.02
0.015
0.6
0.75-1.6
20-23
balance
<0.5
≤1.0
Cr15Ni60
0.08
0.02
0.015
0.6
0.75-1.6
15-18
55-61
<0.5
balance
Cr20Ni35
0.08
0.02
0.015
1.0
1-3
18-21
34-37
-
balance
Cr20Ni30
0.08
0.02
0.015
1.0
1-3
18-21
30-34
-
balance
 

nickel chromium ni80cr20 nikrothal 80 alloy heating element ribbonnickel chromium ni80cr20 nikrothal 80 alloy heating element ribbonnickel chromium ni80cr20 nikrothal 80 alloy heating element ribbonnickel chromium ni80cr20 nikrothal 80 alloy heating element ribbonnickel chromium ni80cr20 nikrothal 80 alloy heating element ribbonnickel chromium ni80cr20 nikrothal 80 alloy heating element ribbon