China Refractory Brick Fused Cast Azs Brick Oxidized Fused Cast Azs Bricks, Find details about China Azs Refractory Brick, Azs Refractory from Refractory Brick Fused Cast Azs Brick Oxidized Fused Cast Azs Bricks
Item | RS-AZS-33 | RS-AZS-36 | RS-AZS-41 | |
ZrO2 % ≥ | 32 | 35 | 40 | |
SiO2 % ≤ | 16.0 | 13.5 | 13.0 | |
Fe2O3 +TiO2+CaO+MgO+K2O+Na2O+B2O3 ≤ | 2.5 | 2.5 | 2.5 | |
Glass phase permeation temperature ºC | 1400 | 1400 | 1400 | |
Bulk density g/cm3 | Ordinary casting ≥ | 3.40 | 3.45 | 3.55 |
Dense casting ≥ | 3.50 | 3.60 | 3.70 | |
No shrinkage cavity casting ≥ | 3.60 | 3.70 | 3.80 |