China Tbm High Performance Steel Cord Conveyor Belting, Find details about China Conveyor Belt, Steel Cord from Tbm High Performance Steel Cord Conveyor Belting
Type | ST1000 | ST1250 | ST1600 | ST2000 | ST2500 | ST3150 | ST3500 | ST4000 | ST4500 | ST5000 | ST5400 |
Tensile strength(N/mm) | 1000 | 1250 | 1600 | 2000 | 2500 | 3150 | 3500 | 4000 | 4500 | 5000 | 5400 |
Steel cord Max. Nominal diameter(mm) | 4.1 | 4.9 | 5.6 | 5.6 | 7.2 | 8.1 | 8.6 | 8.9 | 9.7 | 10.9 | 11.3 |
Pitch of Cord(mm) | 12±1.5 | 14±1.5 | 15±1.5 | 12±1.5 | 15±1.5 | 15±1.5 | 15±1.5 | 15±1.5 | 16±1.5 | 17±1.5 | 17±1.5 |
Thickness of Top Cover(mm) | 4 | 4 | 4 | 4 | 5 | 5.5 | 6.5 | 7 | 7.5 | 8 | 9 |
Thickness of Bottom Cover(mm) | 4 | 4 | 4 | 4 | 5 | 5.5 | 6.5 | 7 | 7.5 | 8 | 9 |
Width(mm) / tolerance | Cord Number | ||||||||||
500 ±5 | 39 | 34 | |||||||||
650 ±7 | 51 | 44 | |||||||||
800 ±8 | 64 | 55 | 50 | 64 | |||||||
1000 ±10 | 81 | 69 | 64 | 81 | 64 | 64 | 64 | 64 | 59 | 55 | 55 |
1200 ±10 | 97 | 84 | 77 | 97 | 77 | 77 | 77 | 77 | 71 | 66 | 66 |
1400 ±12 | 114 | 98 | 90 | 114 | 90 | 90 | 90 | 90 | 84 | 78 | 78 |
1600 ±12 | 131 | 112 | 104 | 131 | 104 | 104 | 104 | 104 | 96 | 90 | 90 |
1800 ±14 | 147 | 127 | 117 | 147 | 117 | 117 | 117 | 117 | 109 | 102 | 102 |
2000 ±14 | 164 | 141 | 130 | 164 | 130 | 130 | 130 | 130 | 121 | 113 | 113 |
2200 ±15 | 181 | 155 | 144 | 181 | 144 | 144 | 144 | 144 | 134 | 125 | 125 |
2400 ±15 | 197 | 169 | 157 | 197 | 157 | 157 | 157 | 157 | 146 | 137 | 137 |
2600 ±15 | 214 | 184 | 170 | 214 | 170 | 170 | 170 | 170 | 159 | 149 | 149 |
2800 ±15 | 231 | 198 | 170 | 214 | 170 | 170 | 170 | 170 | 159 | 149 | 149 |
3000 ±15 | 247 | 212 | 197 | 247 | 197 | 197 | 197 | 197 | 184 | 172 | 172 |
3200 ±15 | 264 | 227 | 210 | 264 | 210 | 210 | 210 | 210 | 196 | 184 | 184 |
Mining Conveyor Belt | Lump Size | Temperatrure of Materials Carried | Belt Surface Temperature |
Coke | 100~200mm(4~8 inch) | 70~100 ºC | 50~60 ºC |
Cement | Powder | 100~250 ºC | 80~90 ºC |
Clinker | 10~30 mm (0.4~1.2 inch) | 100~220 ºC | 100~110 ºC |
Molding | -- | 200~250 ºC | 80~90 ºC |
Metal Powder | -- | 170 ºC | 120~130 ºC |
Raw Material | below 30mm(1.2 inch) | 180~220 ºC | 100~120 ºC |
Sintered Ore | 25~200 mm(1~8i nch) | 200~400 ºC | 130~150 ºC |
Return of Sintered Ore | below 10mm(0.4 inch) | 260 ºC | 180~200 ºC |