Burning-Through Resistant Conveyor Belting

China Burning-Through Resistant Conveyor Belting, Find details about China Conveyor Belt, Rubber Conveyor Belt from Burning-Through Resistant Conveyor Belting

Model NO.
EP100~EP400, NN100~NN400 etc
Thickness
3~30mm
Width
500~2000mm
Tensile Strengeth (MPa)
8~25
Materials
Cement, Coal Mine, Steel, Iron, Quarry etc
Trademark
Jiuzhou
Transport Package
General Packing
Specification
GB, DIN
Origin
Baoding City, Hebei, China
HS Code
40101200
Model NO.
EP100~EP400, NN100~NN400 etc
Thickness
3~30mm
Width
500~2000mm
Tensile Strengeth (MPa)
8~25
Materials
Cement, Coal Mine, Steel, Iron, Quarry etc
Trademark
Jiuzhou
Transport Package
General Packing
Specification
GB, DIN
Origin
Baoding City, Hebei, China
HS Code
40101200
Application :
       The  burning-through  resistant  conveyor  belt  can  be widely  used  in  metallurgical, casting,cement and chemical  industries  for conveying  of  materials  whose  temperature can  reach  150-250

Feature: 
       The  reinforcement  ply  of  the  belt  used  by  the special  glass-fibre,(called  GF fabric  )  .It  is  heat  resistant   is  good  . The  conveyor  belt  has  excellent  stability  and  high -heat  resistant  ,so  the  belt  service   life  is  prolonged.
Type  of   Fabric Reinforcement  D.S EPcover  thickness(mm)No  of  ply width  range (mm)
 GF EP Strength of  Mono  Ply  N/mm top bottom GF DSEP 
 GF D.SEP100 100 >=7 >=3 1 2-6 450-2800
 GF D.SEP150 150  >=7 >=3 1  2-6 450-2800
 GF D.SEP200 200  >=7 >=3 1  2-6 450-2800
 GF D.SEP250 250  >=7 >=3 1  2-6 450-2800
 GF D.SEP300 300  >=7 >=3 1  2-6 450-2800
 GF D.SEP350 350  >=7 >=3 1  2-6 450-2800
 GF D.SEP400 400  >=7 >=3 1  2-6 450-2800
 
Cover Layer Physical Properties After Thermal Aging Test
                                                               Item                          Type
  Type1  Type2  Type3  Type4
                   Changing scope
HardnessDifferences of before and after aging test    +20    ±20    ±20    ±20
Max. after aging test     85    85     85     85
Tensile strength Properties changing rate reducing    -25    -30    -40    -40
Min. after aging test     12     10      5 
Elongation    at breakingChanging rate of properties    -50    -50    -55    -55
Min. after aging test    200    200    180    180
Note: Aging test (100°Cx168h, 125°Cx168h, 150°Cx168h)
Burning-Through Resistant Conveyor BeltingBurning-Through Resistant Conveyor BeltingBurning-Through Resistant Conveyor BeltingBurning-Through Resistant Conveyor Belting