China Metallized BOPET Film 8mic 10mic 12mic for Paperboard′s Lamination, Find details about China Metallized Aluminum Pet Film, Metallized Mylar Film from Metallized BOPET Film 8mic 10mic 12mic for Paperboard′s Lamination
Test Item | Unit | Standard | Test Method | |
Thickness Tolerance | % | ±5 | ASTM D-374 | |
Tensile strength | MD | mpa | ≥200 | ASTM D-882 |
TD | ≥200 | |||
Elongation at break | MD | % | ≥100 | ASTM D-882 |
TD | ≥100 | |||
Heat shrinkage (150ºC,30min) | MD | % | ≤3.0 | ASTM D-1204 |
TD | ≤3.0 | |||
Surface Tension | mN/m | ≥52 | ASTM D-2578 | |
Friction Coefficient | -- | ≤0.80 | ASTM D-1894 | |
≤0.80 | ||||
Base Film Haze | % | ≤3.0 | ASTM D-1003 | |
Thickness of Aluminum Layer | Å | 380 | Square resistance meter | |
Ω/ | 1.50 | GB/T 15717 | ||
O.D | 1.80 | X-rite 361 | ||
Uniformity of Aluminum Layer | % | ±10 | GB/T 15717 | |
Firm of Aluminum Layer | % | 0 | 3M Tape |