3.2 / 4.0mm Solar Glass

China 3.2 / 4.0mm Solar Glass, Find details about China Glass, Solar Glass from 3.2 / 4.0mm Solar Glass

Model NO.
3.2mm / 4mm
Processing Method
Surface Coating
Preparation Process
Sol-Gel Method
Color
Clear
Usage
Solor Glass Panel, Solar Water Heater
Application
Electronics & Instruments
Means of Transportation
Sea, Train, Air
Thickness
3.2mm, 4mm
Size
as Request
Trademark
Sunny Glass
Transport Package
Seaworthy Wooden Crates
Specification
as request
Origin
Shandong, China
HS Code
70071900
Model NO.
3.2mm / 4mm
Processing Method
Surface Coating
Preparation Process
Sol-Gel Method
Color
Clear
Usage
Solor Glass Panel, Solar Water Heater
Application
Electronics & Instruments
Means of Transportation
Sea, Train, Air
Thickness
3.2mm, 4mm
Size
as Request
Trademark
Sunny Glass
Transport Package
Seaworthy Wooden Crates
Specification
as request
Origin
Shandong, China
HS Code
70071900
3.2 / 4.0MM Solar Glass Panel / Building Glass: 
3.2 / 4.0mm Solar Glass


Temperable:  Solar glass
Thickness range: thickness: 2.0~6.0mm 
Iron content:< 100ppm
Solar direct transmission:
 ≥93%(2mm&2.5mm)    ≥91.6%(3.2mm)     ≥91% (4mm)


Tempered size:   Min.:100*300mm    Max.:1650*2200mm
 
Sheet size: 
 Standard Size:1645*987     1574*802    1700*2440    2140*2440
 Max.Size:2140*3700mm (Note: not available for all the thickness) 
   
Application: a-Si Thin Film Solar Cells,cover glass for Silicon Solar panel,solar collector,Solar Water Heaters, BIPV,

 




Features


This kind of glass has the characteristics of high solar transmittance, low absorbance, low reflectance, low iron content, high stability and high safety factor, etc.


3.2 / 4.0mm Solar Glass

Packing
1.Interlay paper between two sheets.
2.Seaworthy wooden crates.
3.Iron/Plastic belt for consolidation 



Specification and parameter
Standard Thickness 3.2mm and 4mm
 Thickness Tolerance 3.2+-0.20mm; 4.0mm+-0.30mm;
 Max size 2250mm*3300mm
 Solar Transmittance (3.2mm) ≥ 91.6%
 Iron Content ≤ 120ppm Fe2O3
 Poisson's Ration 0.2
 Density2.5g/CC 
 Young's Modulus  73. Gpa
 Tensile Strength 42MPa
 Hemispherical Emissivity  0.84
 Epansion Coefficient 9.03*10-6/º C
 Softening Point 720º C
  Annealing Point 550º C