Items | Test Methods | Units | Typical Value | |
Thickness | GB 6672 | μm | 7 | |
Ave. Variation of Thickness | GB/T13541 | % | +0.2 | |
Tensile strength (MD/TD) | GB 13022 | MPa | 160/280 | |
Elongation at Break (MD/TD) | GB 13022 | % | 145/50 | |
Heat Shrinkage (MD/TD) | MP-1 | GB 12026 | % | 3.5/0.5 |
MP-H | 3.0/0.1 | |||
Density | GB 1033 | g/cm3 | 0.91 | |
Surface Roughness(in/out) | GB/T13541 | μm | 0.08/0.08 | |
Wet Tension (Treated Side) | GB/T 14216 | mN/m | 40 | |
Dielectric Strength(Ave/Min)DC | GB/T13541 | V/μm | 496/406 | |
Dielectric Constant | GB/T 13541 | -- | 2.2 | |
Dielectric Consumed Angle tangent | GB/T 13541 | -- | 2.0×10-4 | |
Volume Resistivity | GB/T 13541 | Ω·m | 1.9×1015 |
Items | Units | Typical Value | ||
Thickness | μm | 15 | ||
Ave. Variation of Thickness | % | +0.2 | ||
Tensile strength (MD/TD) | MPa | 155/258 | ||
Elongation at Break (MD/TD) | % | 125/49 | ||
Heat Shrinkage (MD/TD) | % | 3.0/0.3 | ||
Voidage | Average | % | 10.6 | |
Max. | 11.1 | |||
Min | 10.1 | |||
Dielectric Strength DC | Average | V/μm | 550 | |
Min. | 515 | |||
Electric strength (d.c. test) | Central value | V/μm | 356 | |
Not more than 1 of 21 results shall be below | 305 | |||
Dielectric Constant | -- | 2.2 | ||
Dissipation factor | -- | 2.0×10-4 | ||
Volume Resistivity | Ω·m | 3.2×1015 | ||
Surface Roughness(In/Out) | Ra | μm | 0.42/0.40 |