China Compound Dacron Mylar Dacron Fabric 6641 DMD Laminated Insulation Paper Electrical Motor Winding DMD Paper for Motor Winding, Find details about China Insulation Paper, Insulation Materials from Compound Dacron Mylar Dacron Fabric 6641 DMD Laminated Insulation Paper Electrical Motor Winding DMD Paper for Motor Winding
Technical Specification | Unite | Values | |||||||||||||||
Thickness | mm | 0.15 | 0.18 | 0.20 | 0.23 | 0.25 | 0.30 | 0.35 | 0.40 | 0.45 | |||||||
Thickness Tolerance | mm | ±0.02 | ±0.025 | ±0.03 | ±0.03 | ±0.03 | ±0.03 | ±0.035 | ±0.040 | ±0.045 | |||||||
Nominal Grammage and tolerance | g/ | 140±20 | 190±28 | 220±33 | 260±39 | 300±45 | 350±52 | 425±63 | 500±75 | 560±84 | |||||||
Thickness of polyester film | mm | 0.05 | 0.075 | 0.10 | 0.125 | 0.15 | 0.19 | 0.25 | 0.3 | 0.35 | |||||||
Tensile Strength | MD | No Bending | N/10 mm Width | ≥80 | ≥120 | ≥140 | ≥180 | ≥190 | ≥270 | ≥320 | ≥340 | ≥370 | |||||
After Bending | ≥80 | ≥105 | ≥120 | ≥150 | ≥170 | ≥200 | ≥300 | ≥320 | ≥350 | ||||||||
TD | No Bending | ≥80 | ≥105 | ≥120 | ≥150 | ≥170 | ≥200 | ≥300 | ≥320 | ≥350 | |||||||
After Bending | ≥70 | ≥90 | ≥100 | ≥120 | ≥130 | ≥150 | ≥200 | ≥220 | ≥250 | ||||||||
Elongation | MD | No Bending | ≥15 | ||||||||||||||
After Bending | ≥10 | ≥5 | ≥3 | ||||||||||||||
TD | No Bending | ≥20 | |||||||||||||||
After Bending | ≥10 | ≥5 | ≥2 | ||||||||||||||
Breakdown Voltage | KV | ≥6 | ≥7 | ≥9 | ≥10 | ≥12 | ≥15 | ≥18 | ≥20 | ≥22 | |||||||
Bond strength at 25 degree C | No delamination | ||||||||||||||||
Bond strength at 180 degree C | No delamination,no blister,no adhesive flow | ||||||||||||||||
Temperature | 155 |