Grade33 ( 230 ) Gl Galvalume Steel coil with Anti-Finger Print

China Grade33 (230) Gl Galvalume Steel coil with Anti-Finger Print, Find details about China Gl, Gl Aluzinc Steel in Coil from Grade33 (230) Gl Galvalume Steel coil with Anti-Finger Print

Model NO.
SPCC, SPCD
Stock
Not Stock
Name
Galvalume Steel Coil
Grade
230
Sample
Available
Yield Strength
230
Tensile Strength
310
Width
600-1250mm
Thickness
0.15-3.0mm
Payment
30%Deposit, 70% See Copy of B/L
Delivery
15-40days
Coil Weight
3-8tons
Trademark
Dinggang or as customer′s request
Transport Package
Strandard Export Packing
Specification
JIS G 3321-2e
Origin
China
HS Code
72106100
Model NO.
SPCC, SPCD
Stock
Not Stock
Name
Galvalume Steel Coil
Grade
230
Sample
Available
Yield Strength
230
Tensile Strength
310
Width
600-1250mm
Thickness
0.15-3.0mm
Payment
30%Deposit, 70% See Copy of B/L
Delivery
15-40days
Coil Weight
3-8tons
Trademark
Dinggang or as customer′s request
Transport Package
Strandard Export Packing
Specification
JIS G 3321-2e
Origin
China
HS Code
72106100
Feature of the aluzinc steel:
1. Standard of Aluzinc Steel: ASTM A 792
2. Surface treatment of Aluzinc Steel: Chromated. Oiled, bright finish, fingerprint resistance
3. Thickness of Aluzinc Steel: 0.2mm-1.2mm
4. Width of Aluzinc Steel Coil: 600mm-1 250mm, our normal width: 1000 mm, 1200mm, 1250 mm
5. Coating weight of Aluzinc Steel: AZ50, AZ100, AZ150
6. Coil weight: As per customers' requests, 3-5 tons per coil generally
7. ID: 508mm.
8. Standard export packing
9. Applications: General use, construction industry, household appliance industry, automobile industry and industrial instruments
Package: Fancy package or as per customers' requests
10. Original: China

Aluminium-zinc alloy armor plate, is called Al-Zn coated plate for short Strips, after through three processes, including payoff reel, crop shear and welding, enter into the continuous annealing furnace. During the annealing process, strips are heated closer to the recrystallizing temperature, and then heated to 20~50º C above the recrystallizing temperature in the reducing furnace. After keeping the same temperature for 170s, strips are naturally cooled to the normal temperature in the slow cooling process. Afterward, strips enter into the zinc pot through the elephant's trunk and begin in the hot-dip coating process. The optimum temperature range of the plating coat is 630º C~660º C. Coated with aluminium-zinc alloy, strips enter into the cooling tower by the steady roll and air knife. After fast cooled with wind or water, they are directly produced into Al-Zn armor plates. The general rate of cooling is 30º C/s or so, and strips are cooled to about 60º C.
Chemical Requiremetns for structure steel
Composition, %-Heat Analysis Element, maximum, unless otherwise Shown
DesignationCMnPSCuNiCrMoVCbTiANB
G2300.201.350.040.040.250.200.150.060.0080.0080.025^
G2550.201.350.100.040.250.200.150.060.0080.0080.025^
G2750.251.350.100.040.250.200.150.060.0080.0080.025^
G3400.251.350.200.040.250.200.150.060.0080.0080.025^
G5500.201.350.040.040.250.200.150.060.0080.0150.025^