Attribute | Zirconia | Alumina | ZTA |
Density | 5.9-6.05g/cm3 | 3.6-3.8g/cm3 | 4.8g/cm3 |
Hardness(HRC) | 88-90 | 80-86 | 86 |
Fracture Toughness | 10MPa.m½ | 4MPa.m½ | - |
Compressive Strength | 2000MPa | 1500MPa | 1700MPa |
CTE | 10.5ppm/ºC | 7.15-7.67ppm/ºC | 9.1ppm/ºC |
Maximum Operating Temperature | 1350ºC | 1700ºC | 1350ºC |
Thermal Conductivity(24ºC) | 2W/m.k | 18-28W/m.k | - |
Flexural Strength (24ºC) | 950MPa | 300MPa | 600MPa |
Water Absorption(%) | 0 | 0 | 0 |