BOPP Thermal Lamination Film-Glossy 25micron

China BOPP Thermal Lamination Film-Glossy 25micron, Find details about China BOPP Laminating Film, BOPP Film from BOPP Thermal Lamination Film-Glossy 25micron

Model NO.
BG1509
Thickness
24mic
Width
300-1770mm
Length
200-3000m
Paper Core
1inch 2.25inch 3inch
Item
Gloss and Matt
Trademark
FSEKO
Specification
305mm, 457mm, 635mm
Origin
Guangdong, China
HS Code
3920
Model NO.
BG1509
Thickness
24mic
Width
300-1770mm
Length
200-3000m
Paper Core
1inch 2.25inch 3inch
Item
Gloss and Matt
Trademark
FSEKO
Specification
305mm, 457mm, 635mm
Origin
Guangdong, China
HS Code
3920
*About EKO
FSEKO has been in the field of lamination film for over 10 years. And the quality is controlled by the quality system ISO 9001: 2008.
 
*Material
Surface layer: BOPP
Glue layer: EVA adhesive

*Specification                          
 

SPECIFICATION & PARAMETER
SPECIFICATION20G
GLOSS
22G
GLOSS
25G
GLOSS
27G
GLOSS
23M
MATT
24M
MATT
25M
MATT
27M
MATT
30VM
VELVET MATT
THICKNESS
(μm )
TOTAL202225272324252730
base121215151512151519
glue8101012812101211
WEIGHTm 2 /kg54.349.343.3840.1148.2646.5544.2541.0038.30
kg/m 20.018440.020320.023050.024930.020720.021480.02260.02440.02612
WIDTH(mm)360 390 440 540 590 780 880 1080 1320 1400 1600 1800
(or as customers'requset)     
LENGTH(m)200-3000
PAPER CORE25.4mm(1 inch)\58mm(2.25 inch)\76mm(3 inch)
BONDINGLESS THAN 2
TENSILE
STRENGTH
MD:2.4×10 6 dyne/cm     CD:5.3×10 6 dyne/cm

 

Certificate
1. SGS
2. ISO9001: 2008
Process Parameter:
Equipment:dry or wet film laminator
Temperature:Normal:85-100 degree
Special:100-110 degree
Roller Pressure:10-18Mpa
Speed:8-50m/min
Remarks:Special laminations refer to those with thicker ink,solid color,high moisture content and bigger size paper.
 
 
 
*directions for using BOPP thermal laminating film:
Normal process temperature is 90c-105c, roller pressure and temperature vary
with different types of paper, ink and machines.
When using the film for the first time or do other treatment, try a small volume 
before mass laminating.
Make sure the ink is dry before laminating. It will delaminate when the paper 
contains too much moisture and powder.
Make sure put the material in a low-temperature, dry place.

*The delivery deadline
25 days according the order quantity


*Packing:
Standard export packing is Rolling package with cartons; In pallet individual corrugated boxes;