China Flat Heating Wire Heating Nichrome Wire Heating Wire Ni80Cr20 (N80), Find details about China kanthal wire, heating resistant wire from Flat Heating Wire Heating Nichrome Wire Heating Wire Ni80Cr20 (N80)
Condition | Bright / Acid White / Oxidied Color |
Diameter | 0.018mm-1.6mm in Spool, 1.5mm-8mm in Coil, 8mm-60mm in Rod |
Round Wire Diameter | 0.018mm - 10mm |
Ribbon | Thickness 0.01-2mm, Width 0.5-5mm |
Strip | Thickness 0.001-7mm, Width 1-450mm |
Grade | 1Cr13Al4, 0Cr25Al5, 0Cr21Al6, 0Cr23Al5, 1Cr20Al3, 0Cr21Al6Nb, 0Cr27Al7Mo2 |
Production Standard | ASTM B603, DIN 17470, JIS C2520, GB/T 1234 |
Characteristics | Stable Performance, Anti-Oxidation, Corrosion Resistance, High Temperature Stability, Excellent Coil-Forming Ability, Uniform and Beautiful Surface Condition without Spots |
Usage | Resistance Heating Elements; Material in Metallurgy; Household Appliances; Mechanical Manufacturing and other industries. |
Nichrome's metallurgical structure confers them a very good plasticity when cold | |
Our Advantages | High Quality, Short Delivery Time, Small MOQ |
Alloy Nomenclature Performance | 1Cr13Al4 | 0Cr25Al5 | 0Cr21Al6 | 0Cr23Al5 | 1Cr20Al3 | 0Cr21Al6Nb | 0Cr27Al7Mo2 | |
---|---|---|---|---|---|---|---|---|
Main Chemical composition | Cr | 12.0-15.0 | 23.0-26.0 | 19.0-22.0 | 20.5-23.5 | 18.0-21.0 | 21.0-23.0 | 26.5-27.8 |
Al | 4.0-6.0 | 4.5-6.5 | 5.0-7.0 | 4.2-5.3 | 3.0-4.2 | 5.0-7.0 | 6.0-7.0 | |
Re | opportune | opportune | opportune | opportune | opportune | opportune | opportune | |
Fe | Rest | Rest | Rest | Rest | Rest | Rest | Rest | |
Nb0.5 | Mo1.8-2.2 | |||||||
Max. continuous service temp. of element | 950 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 | |
Resistivity at 20ºC (μΩ·m) | 1.25 | 1.42 | 1.42 | 1.35 | 1.23 | 1.45 | 1.53 | |
Density (g/cm3) | 7.40 | 7.10 | 7.16 | 7.25 | 7.35 | 7.10 | 7.10 | |
Thermal conductivity(KJ/m·h·ºC) | 52.7 | 46.1 | 63.2 | 60.2 | 46.9 | 46.1 | 45.2 | |
Coefficient of lines expansion(α×10-6/ºC) | 15.4 | 16.0 | 14.7 | 15.0 | 13.5 | 16.0 | 16.0 | |
Melting point (approx.)( ºC) | 1450 | 1500 | 1500 | 1500 | 1500 | 1510 | 1520 | |
Tensile strength (N/mm2) | 580-680 | 630-780 | 630-780 | 630-780 | 600-700 | 650-800 | 680-830 | |
Elongation at rupture (%) | >16 | >12 | >12 | >12 | >12 | >12 | >10 | |
Variation of area(%) | 65-75 | 60-75 | 65-75 | 65-75 | 65-75 | 65-75 | 65-75 | |
Bending frequency (F/R) | >5 | >5 | >5 | >5 | >5 | >5 | >5 | |
Hardness(H.B.) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | |
Continuous Service Time(Hours/ ºC) | -- | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥80/1350 | ≥80/1350 | |
Micrographic structure | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | |
Magnetic properties | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic |