A Nickel-Chromium-Cobalt alloy being precipitation hardenable, having high stress-rupture strength and creep resistance at high temperatures up to about 950oC (1740oF). It is widely used and a well proven alloy in high temperature conditions.
Chemical CompositionSpecificationsDesignationsKey FeaturesTypical Applications
ElementMin %Max %
Nibal
Cr18.0021.00
Fe-1.50
Ti2.003.00
Mn-1.0
Si-1.0
C-0.13
Al1.002.00
Co15.0021.00
S-0.015
Cu-0.20
B-0.02
Pb-0.002
Zr-0.15
Ag-0.0005
Bi-0.0001
AMS 5829
BS HR 501
BS HR 502
BS HR 503
BS 3075 NA 19
ISO 15156
(NACE MR 0175)
NCK 20TA
W.Nr 2.4632
W.Nr 2.4969
UNS N07090
AWS 030
High stress rupture strength and high creep resistance at high temperatures
Good resistance to high-temperature corrosion and oxidation
Age hardenable
High temperature dynamic applications
Aerospace fasteners
Density8.18g/cm³0.296 lb/in³
Melting Point1370°C2500°F
Coefficient of Expansion12.7 μm/m °C (20 - 100°C)7.1 x 10-6 in/in °F (70 - 212°F)
Modulus of Rigidity82.5 kN/mm²11966 ksi
Modulus of Elasticity
(Annealed + Aged)
(Spring Temper + Aged)
213 kN/mm²
227 / 240 kN/mm²
30894 ksi
32924 / 34810 ksi
Heat Treatment of Finished Parts
Condition as supplied by Alloy WireTypeTemperatureTime (Hr)Cooling
°C°F
AnnealedAge Harden75013804Air
Spring TemperAge Harden65012004Air
Spring TemperAge Harden600111016Air
Properties
ConditionApprox. tensile strengthApprox. operating temperature
N/mm²ksi°C°F
Annealed800 - 1000116 - 145--
Annealed + Aged1200 - 1400174 - 203up to 550up to 1020
Spring Temper1300 - 1500189 - 218--
Spring Temper + Aged1500 - 1800218 - 261up to 350up to 660

The above tensile strength ranges are typical. If you require different please ask.