China Rare Earth Sm2co17 Magnets, Find details about China Permanent Samarium Cobalt Magnets, Sintered Smco Magnets from Rare Earth Sm2co17 Magnets
Material | Code | Remanence Br | Coercivity Force | Intrinsic Coercivity | Maximum Energy | Curie | Maximum Operating | ||||
Force | Product Bhm | Temperature | Temperature | ||||||||
Br | bHc | iHc | (BH)max | TC | TW | ||||||
T | KGs | KA/m | KOe | KA/m | KOe | KJ/m 3 | MGOe | ° C | ° C | ||
Sintered | |||||||||||
YX-18 | 0.85-0.9 | 8.5-9.0 | 620-648 | 7.8-8.2 | 1194-1513 | 15-19 | 127-143 | 16-18 | 750 | 250 | |
SmCo1: 5 | YX-20 | 0.92-0.96 | 9.2-9.6 | 653-717 | 8.2-9.0 | 1194-1513 | 15-19 | 150-167 | 19-21 | 750 | 250 |
YX-24 | 0.96-1.0 | 9.6-10.2 | 730-770 | 9.2-9.7 | 1194-1513 | 15-19 | 175-190 | 22-24 | 750 | 250 | |
YXG-24 | 0.95-1.02 | 9.5-10.2 | 637-732 | 8.0-9.2 | 1433-1990 | 18-25 | 175-190 | 22-24 | 800 | 350 | |
smCo2: 17 | YXG-26 | 1.02-1.05 | 10.2-10.5 | 748-796 | 9.4-10.0 | 1433-1990 | 18-25 | 195-215 | 24-26 | 800 | 350 |
YXG-28 | 1.05-0.08 | 10.5-10.8 | 756-796 | 9.5-10.0 | 1433-1831 | 18-25 | 205-220 | 26-28 | 800 | 350 | |
YXG-28B | 1.02-1.10 | 10.2-11.0 | 420 | 5.2-5.6 | 440-520 | 5.5-6.5 | 205-220 | 26-28 | 800 | 350 | |
YXG-30 | 1.08-1.10 | 10.8-11.0 | 780 | 9.8-10.5 | 955-1195 | 18-25 | 220-240 | 28-30 | 800 | 350 | |
YXG-30B | 1.08-1.15 | 10.8-11.5 | 420 | 5.2-5.6 | 440-520 | 5.5-6.5 | 220-240 | 28-30 | 800 | 350 | |
Bonded | |||||||||||
Yb-6 | 0.4 | 4.0 | 280 | 3.5 | 800 | 10 | 30-50 | 4-6 | - | 120 | |
smCo1: 5 | Yb-10 | 0.5 | 5.0 | 320 | 4.0 | 800 | 10 | 50-65 | 6-8 | - | 120 |
YbG-10 | 0.6 | 6.0 | 360 | 4.5 | 800 | 10 | 65-80 | 8-10 | - | 120 | |
smCo2: 17 | YbG-12 | 0.7 | 7.0 | 400 | 5.0 | 800 | 10 | 85-95 | 10-12 | - | 120 |