Customizing Steel Lined LLDPE PTFE Pipe with Chemical Discharge PTFE Lined F46 Valves

China Customizing Steel Lined LLDPE PTFE Pipe with Chemical Discharge PTFE Lined F46 Valves, Find details about China Lined PTFE Pipe, Steel Lined PE Pipe from Customizing Steel Lined LLDPE PTFE Pipe with Chemical Discharge PTFE Lined F46 Valves

Model NO.
Steel Lined LLDPE PTFE Pipe
Usage
Pipeline Transport, Boiler Pipe, Hydraulic/Automobile Pipe, Oil/Gas Drilling, Food/Beverage/Dairy Products, Machinery Industry, Chemical Industry, Mining, Construction & Decoration, Special Purpose
Section Shape
Round
Materical
Q235A + PE F46 PTFE(Plastic )16mm -22mm
Trademark
Dong Run Ze
Transport Package
Nil
Specification
OEM
Origin
China
HS Code
73090000
Model NO.
Steel Lined LLDPE PTFE Pipe
Usage
Pipeline Transport, Boiler Pipe, Hydraulic/Automobile Pipe, Oil/Gas Drilling, Food/Beverage/Dairy Products, Machinery Industry, Chemical Industry, Mining, Construction & Decoration, Special Purpose
Section Shape
Round
Materical
Q235A + PE F46 PTFE(Plastic )16mm -22mm
Trademark
Dong Run Ze
Transport Package
Nil
Specification
OEM
Origin
China
HS Code
73090000
Customizing Steel Lined LLDPE PTFE  Pipe  With Chemical Discharge PTFE Lined F46 Valves 

Anticorrosive Steel Lined Plastic PTFE ,LLDPE  Pipe Use for  Sulfuric Acid Hydrochloric Acid  HCL, NaOH, NaCLO,
Steel lined piping with tetrafluoride
Molded piping with tetrafluoride
Anticorrosive pipeline resistant to high temperature and negative pressure
Chemical pipeline


Metal cans Steel-Lined Plastic Square Tank, Electrolytic Tank, Pickling Tank  Acid Containment Vessels Custom Made Rotationally Molded Linear Resins LLDPE
Custermizing Checmial Acid Storage Tank 60 m3 Steel Lined LLDPE  Tank Used to Contain: HCl (max 35%) , Naoh (max 50%) , Naclo (max 10%) , PAC (max 17%) ,H2so4  

Used to contain: HCl (max 35%), NaOH (max 50%), NaCLO (max 10%), PAC (max 17%), H2SO4 etc 


 Media (density) : (1155 Kg/m3), Hydrochloric Acid (1150 Kg/m3), Sulfate, Nitrate (1152 Kg/m3), Phosphate (1151 Kg/m3), Hydrofluoric Acid (1132 Kg/m3), Battery Fluid (1135 Kg/m3), Chloride (1135 Kg/m3), Ferric Chloride Solution (1130 Kg/m3), Sodium Hypochlorite (1130 Kg/m3), Sulfurous Acid (1030 Kg/m3)

processing/storing; aluminum sulfate, ammonium sulfate, calcium chloride, ethylene glycol, ferric chloride, ferric sulfate, ferrous sulfate, hydrochloric acid, hydrofluoric acid, hydrofluosilicic acid, hydrogen peroxide, magnesium chloride, phosphoric acid, polymers, potassium hydroxide, or just plain water and we'll design the vessel(s) you require.

Horizontal / Vertical Storage HCL Acid Tanks Steel Lined LDPE 120000 Liters 
For Storage Bleach, Hydrochloric Acid, Ferric Chloride, Oilfield Chemicals, Corrosive Wastes And Other Hazardous Cargoes. 
Steel ( 6 mm -8mm ) Lined PE Plastic 7042 (16mm - 25 mm ) storage tank

Detail Picture
 

Customizing Steel Lined LLDPE PTFE Pipe with Chemical Discharge PTFE Lined F46 Valves
Customizing Steel Lined LLDPE PTFE Pipe with Chemical Discharge PTFE Lined F46 Valves
Customizing Steel Lined LLDPE PTFE Pipe with Chemical Discharge PTFE Lined F46 Valves

Customizing Steel Lined LLDPE PTFE Pipe with Chemical Discharge PTFE Lined F46 Valves
Customizing Steel Lined LLDPE PTFE Pipe with Chemical Discharge PTFE Lined F46 Valves

Customizing Steel Lined LLDPE PTFE Pipe with Chemical Discharge PTFE Lined F46 Valves

 





Customizing Steel Lined LLDPE PTFE Pipe with Chemical Discharge PTFE Lined F46 Valves

01.Carefully selected seamless steel pipe

02 .Steel pipe Weld Flange and Polishing

03 .Steel pipe Sandblasting 

04 .Steel pipe Lined PE

05 .Steel pipe Cooling,Primer, Topcoat Paint Anti rust
 

SpecificationGeneral PTFE thickness and negative pressure-resistanceThe thickness of PTFE wall required to resist-0.1MPA pressure when the temperature is less than 120degree,
DN252mm-0.08Mpa3mm(L≤3000mm)
DN322mm-0.075Mpa3mm(L≤3000mm)
DN402.5mm-0.075Mpa4mm(L≤3000mm)
DN502.5mm-0.06Mpa5mm(L≤3000mm)
DN652.5mm-0.05Mpa8mm(L≤1000mm)
DN803mm-0.05Mpa10mm(L≤1000mm)
DN1003mm-0.04Mpa13mm(L≤1000mm)
DN1254mm-0.03Mpa13mm(L≤1000mm)
DN1504mm-0.025Mpa13mm(L≤1000mm)
DN2005mm-0.02Mpa15mm(L≤1000mm)
Specifications:
Nominal Diameter (mm/in. ): DN15-DN600 (NPS 1/2-NPS 24)
Operating temperature: -20-180 degree
Operating pressure: -0.09MPa-1.6MPa (-0.9bar-16bar)
Pipe: Seamless steel.
Flange: ASME B16.5 Class 150 Flange options: HG, GB, JB, JIS, BS, DIN, ANSI, ASTM
Special pieces of specific or non standard size can be manufactured on request.

Carbon steel 45/90degree ptfe lined elbow
Operating temperature: -20-180
Operating pressure: -0.09MPa-1.6MPa



Carbon steel 45/90degree ptfe lined elbow
1. Positive pressure: It shall adopt steel components according to different technical requirements, and the thickness of PTFE wall shall be over 2mm. If the temperature is less than 100 degree, the production length shall be less than 6m; And if the temperature exceeds 100 degree, the length shall be less than 3m.
2. Negative pressure: Design according to different ambient conditions of the users
PTFE lined 90° elbow     Unit mm
Nominal diameterSpecification of balled iron TRaised face ACentral height C1Inside diameter D1PTFE thicknessout side diameter of flange DDiameter of bolt circle KThickness of flange C
DN(mm)NPS(inch)
DN151/2344080155906511
DN203/43845901851007511
DN2514260922251108512
DN321 1/4487010028513010013
DN401 1/2578011238514011014
DN502689511748515512514
DN652 1/28911513563817514516
DN80310813015078819016016
DN100411415015087821018018
DN1255140180190110824021020
DN15061682052301351027524020
DN20082192603051801033029520
DN250102733153802301238535023
DN300123253654202801243540023

 

Key words:

ptfe lined pipe fittingsptfe lined teeptfe lined reducerptfe lined elbowptfe lined cross
ptfe lined pipe and fittingsptfe lined90degree elbowptfe lined 45 degrdd elbowptfe lined ECC reducerptfe lined CON reducer
ptfe lined equal teeptfe lined reduce teeptfe lined unequal teeptfe lined pipeptfe lined fittings
ptfe lined carbon steel pipe fittingsptfe lined carbon steel teeptfe lined carbon steel reducerptfe lined carbon steel elbowptfe lined carbon steel cross
PTFE pipe PTFE lined pipe(Australia)   Resistant Stainless Steel PipeResistant Steel PipeCarbon seamless steel pipe
Anti Corrosion Pipe Fittings LinedPTFE lining fittings PTFE lined pipingstraight teePTFE lined bends

 


Rotationally Molded LLDPE TANK
  
 
 tictrucks.en.made-in-china.com   

LDPE / HDPE Chemical Resistance Chart 

The chemical compatibility of LDPE and HDPE on this chart is tested at 20°C: and 50°C: for 7 days and 30 days (if applicable) with constant exposure.

LDPE & HDPE resistance listed by chemical
1.4-dioxaneLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows some effect after 7 days.
AcetaldehydeLDPE / HDPE at 20°C: little or no damage after 30 days.
HDPE at 50°C: shows some effect after 7 days.
LDPE at 50°C: immediate damage may occur.
Acetic Acid 5 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Acetic Acid, glacial 50%LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50 °C: immediate damage may occur.
AcetoneLDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.
Allyl AlcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Aluminum saltsLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Amino acidsLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
AmmoniaLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ammonium carbonate saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ammonium phosphateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ammonium sulphateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Amyl chlorideHDPE at 20°C: shows some effect after 7 days.
HDPE at 50°C & LDPE at 20°C-50°C: immediate damage may occur.
Not recommended for continuous use.
AnilineLDPE / HDPE at 20°C: little or no damage after 30 days.
HDPE at 50°C: shows some effect after 7 days.
BenzeneLDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.
Benzyl alcoholLDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.
Boric acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
BromineLDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.
Butyric acidLDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.
Calcium chlorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Calcium hydroxide saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Carbon tetrachlorideHDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C & HDPE at 50°C: show some effect after 7 days.
LDPE at 50°C: not recommended.
Chlorine 10% in waterLDPE / HDPE at 20°C: shows little or no damage after 30 days.
LDPE at 50°C: shows damage and is not recommended.
ChlorobenzeneImmediate damage may occur.
Not recommended for continuous use.
ChloroformLDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: immediate damage may occur.
Not recommended for continuous use.
Chromic acid 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Chromic acid 50%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Citric acid 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
CresolHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage.
Not recommended for continuous use.
CyclohexaneLDPE / HDPE at 50°C: immediate damage may occur.
LDPE / HDPE at 20°C: show some effect after 7 days.
Diethyl ketoneLDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.
DimethylsulfoxideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethanol 95%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethyl acetateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethyl benzeneHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage.
Not recommended for continuous use.
Ethylene glycolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethylene oxideHDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C: and LDPE/ HDPE at 50°C: show some effect after 7 days.
Ferric chlorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
FluorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
FluorineHDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C: shows some effect after 7 days.
Not recommended at 50°C.
Formaldehyde 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Formaldehyde 40%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
GlycerolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
HexaneHDPE at 20°C: shows little or no damage after 30 days continuous use.
HDPE at 50 °C: shows some effect after 7 days.
LDPE not recommended at any temperature.
Hydrochloric acid 20%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrochloric acid 35%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrochloric acid 5%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrocyanic acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrofluoric acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrofluoric acid 4%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrofluoric acid 48%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrogen peroxide 3%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrogen peroxide 30%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Isobutyl alcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Isopropyl alcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
KeroseneLDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE not recommended at 50°C, as immediate damage may occur.
Lactic Acid 10 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Lactic Acid 90 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Lead acetateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
MethanolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Methyl ethyl ketoneImmediate damage may occur.
Not recommended for continuous use.
Methyl propyl ketoneHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur.
Not recommended for continuous use.
Methylene chlorideHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur.
Not recommended for continuous use.
Mineral oilLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: may show immediate damage and is not recommended.
n-amyl acetateLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows some effect after 7 days or constant exposure.
n-butyl alcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
HNO3 acid 50 %LDPE at 20°C: shows little or damage after 30 days.
HDPE at 20°C & LDPE at 50°C: show effect after 7 days.
HDPE at 50°C: shows immediate damage and is not recommended.
HNO3 acid 70 %LDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
n-octaneLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Oleic acidHDPE at 20°C-50°C: little or no damage after 30 days.
LDPE at 20°C-50°C: shows immediate damage and is not recommended.
Oxalic acidLDPE at 20°C: shows some effect after 7 days.
HDPE at 20°C and LDPE / HDPE at 50°C: shows little/ no damage after 30 days.
OzoneLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
Perchloric acidLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
Perchloric ethyleneLDPE / HDPE at 20°C-50°C: show immediate damage.
Not recommended.
PhenolLDPE / HDPE at 20°C-50°C: show immediate damage.
Not recommended.
Phosphoric acid 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Phosphoric acid 85%LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows immediate damage and is not recommended.
Phosphorous trichlorideLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: has no data available. HDPE at 50°C: shows some effect after 7 days.
Potassium carbonateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Potassium hydroxide 5 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Potassium hydroxide concentratedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Potassium permanganateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Propylene glycolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
PyridineImmediate damage may occur.
Not recommended for continuous use.
Salicylic acid, saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Silver acetateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Silver nitrateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium carbonateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium chloride, saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium dichromateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium hydroxide 1%LDPE at 20°C-50°C: shows little or no damage after 30 days.
HDPE at 20°C-50°C: shows some effect after 7 days.
Sodium hydroxide 50%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium hypochlorite 15%HDPE at 20°C-50°C: little or no damage after 30 days.
LDPE at 20°C: is suitable
 but at 50°C: shows some effect after 7 days.
Sodium nitrateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium sulphateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
SucroseLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 20%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 6%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 60%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 98%LDPE at 20°C-50°C: shows little or no damage after 30 days.
HDPE at 20°C: shows effect after 7 days.
Not recommended for use at 50°C.
Tannic acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
TetrahydrofuranLDPE / HDPE at 20°C: show some effect after 7 day of constant exposure.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
TolueneLDPE at 20°C: show some effect after 7 day of constant exposure.
HDPE at 20°C-50°C & LDPE at 50°C: show immediate damage.
Not recommended.
Trichloracetic acidLDPE / HDPE at 20°C: show some effect after 7 day of constant exposure.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
TrichlorethaneImmediate damage may occur.
Not recommended for continuous use.
Turpentine oilLDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
UreaLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
XyleneHDPE at 20°C: shows some effect after 7 day of constant exposure.
LDPE at 20-50°C and HDPE at 50°C: show immediate damage.
Not recommended.
Zinc chlorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.