Tp20 Wrinkle Agent for Chemical Powder Coating

China Tp20 Wrinkle Agent for Chemical Powder Coating, Find details about China Wrinkle Agent, Powder Coating from Tp20 Wrinkle Agent for Chemical Powder Coating

Model NO.
Tp20
Method
Spray
Components
Organic Metallic Complex
Main Raw Material
Organic Metallic Complex
Level
Finish Coat
Certification
ISO14001, ISO9001
Substrate
Steel
Expiration Date
3 years
Formation Mechanism
Conversion Type
Packaging
Plastic Drum
Trademark
TP
Transport Package
20kgs Per Bag
Specification
20kgs Per Bag
Origin
China
HS Code
2914190090
Model NO.
Tp20
Method
Spray
Components
Organic Metallic Complex
Main Raw Material
Organic Metallic Complex
Level
Finish Coat
Certification
ISO14001, ISO9001
Substrate
Steel
Expiration Date
3 years
Formation Mechanism
Conversion Type
Packaging
Plastic Drum
Trademark
TP
Transport Package
20kgs Per Bag
Specification
20kgs Per Bag
Origin
China
HS Code
2914190090
TP20 WRINKLE AGENT

General Description:

Winkle agent TP20 is also called as watermark agent. It is a kind of metal organic complexes which has a strong effect of curing acceleration, making the gel time very short and the coating has no time for leveling, thus can produce the well distributed wrinkle pattern like ground glass.
After the formula is adjusted, it is can produce sand texture, wrinkles and turtle shell textures.
Tp20 Wrinkle Agent for Chemical Powder Coating
Tp20 Wrinkle Agent for Chemical Powder Coating

Technical Parameters
Item Test Methods Specification
Appearance Visualization Yellowish powder
Melting Range (ºC) GB/T617-2006 190-196
Purity(%) GB/T1725-2007 ≥98.5
Curing Condition 180ºC/20-25min;190ºC/ 15min;200ºC/10-12min.

Application
Used for producing fine wrinkle surface or other art powder such as sand texture and turtle shell texture .

Use method % characteristics
The dosage over 5wt% of the resin mixed with other materials and extruded .in the process of producing wrinkle coatings, the surface form is related to the dosage of TP20 and fillers. The more fillers used, the smaller wrinkle obtained.

Suggested Formulation
Raw material Bottom powder Formula 1 Formula 2 Formula
3 hybrid 7:3 remarks
Epoxy Resin E-12 60wt% 60 60 560-580
Polyester TP4060 3wt% 0 5 N/V Use little 6:4 and 7:3 polyester to make texture big
Dicyandiamide 2.4wt% 3 3 22-24 Dosage :4-5% of epoxy
Wrinkle Agent TP20 3.6wt% 3 3 19-23 Can reduce to 2
Flowing Agent TP88 0.2wt% 0.2% 0.2% 2 Small dosage filler
gets big texture, Vice versa
Pigment and filler 30-50% 30-50% 30-50% 300-
500% Eliminate pitting and bright spots

Extruding temperature: 90-100 °C, sieve through 140 mesh sieve
Due to the strong effect curing  acceleration of TP20, please extruding with low temperature

Take above formulation as base powder, than dry blending 0.1−0.2% TP80( turtle shell texture agent )can obtain turtle shell texture or snow pattern.

Spray thick thickness for big texture, otherwise, the coating will be shining; or spray thin thickness for small texture. Curing condition: 200°C/15min.

Used in hybrid or pure polyester system can get the effect of wrinkle and sand texture.

TP20  can also use as dry blending. Dry blending TP20 will consume smaller dosage compare with extruding, and the texture more coarse.

Try to not breathe the product dust for a long time, or else will arise symptoms feel like common cold. After disengagement of dust exposure, the symptoms will disappear in one week.

Package & Storage & Handling
1.Available in polyethylene-lined, multi-ply paper bags, N.W. 25KGS/Bag.
1.Storage in cool and dry place, avoid contact with skin and eyes; wear dust mask when operating; wash with water after operation.
2.Validity will be 1 years under normal temperature.

Tp20 Wrinkle Agent for Chemical Powder CoatingTp20 Wrinkle Agent for Chemical Powder CoatingTp20 Wrinkle Agent for Chemical Powder CoatingTp20 Wrinkle Agent for Chemical Powder CoatingTp20 Wrinkle Agent for Chemical Powder CoatingTp20 Wrinkle Agent for Chemical Powder CoatingTp20 Wrinkle Agent for Chemical Powder Coating