Constantan Wire/Strip/Bar/Foil/Ribbon Cu56ni44 220V Electric Resistance Wire for Oven Design

China Constantan Wire/Strip/Bar/Foil/Ribbon Cu56ni44 220V Electric Resistance Wire for Oven Design, Find details about China Constantan Nc50 Cuprothal Alloy 294, Alloy 45 CuNi 102 Konstantan Constantan from Constantan Wire/Strip/Bar/Foil/Ribbon Cu56ni44 220V Electric Resistance Wire for Oven Design

Model NO.
SP-OhmAlloy049
Sheath Material
None
Insulation Material
None
OEM
Available
Trademark
Ohmalloy
Transport Package
Wooden Case
Specification
0.06mm~8mm
Origin
China
Model NO.
SP-OhmAlloy049
Sheath Material
None
Insulation Material
None
OEM
Available
Trademark
Ohmalloy
Transport Package
Wooden Case
Specification
0.06mm~8mm
Origin
China
Constantan Wire/Strip/Bar/Foil/Ribbon Cu56Ni44 220v Electric Resistance Wire for Oven Design
 

(Common Name: CuNi45, NC50.Cuprothal, Alloy 294, Cuprothal 294, Nico, MWS-294, Cupron, Copel, Alloy 45, Neutrology, Advance, CuNi 102, Cu-Ni 44, Konstantan,constantan.)

OhmAlloy049 is a copper-nickel alloy (Cu56Ni44 alloy) characterized by high electrical resistance, high ductility and good corrosion resistance. It is suitable for use at temperatures up to 400°C

Typical applications for OhmAlloy49 are temperature-stable potentiometers, industrial rheostats and electric motor starter resistances.

The combination of negligible temperature coefficient and high resistivity makes the alloy particulary suitable for the winding of precision resistors.

OhmAlloy049 is manufactured from electrolytic copper and pure nickel. In finer wire sizes the alloy is designated as OhmAlloy49TC(Thermocouple).


Copper Nickel Alloy Heating Resistance Wire and Strip Technique Data
 

Name

 Our Code

Resistance Ω at 20 °C

the maximum temperature°C

Copper-nickel--1

OhmAlloy3

0.03

200

Copper-nickel--2

OhmAlloy5

0.05

200

Copper-nickel--8

OhmAlloy12 

0.12

250

Copper-nickel--10

OhmAlloy15

0.15

200

Copper-nickel--14

OhmAlloy20

0.2

300

Copper-nickel--19

OhmAlloy25

0.25

300

Copper-nickel--23

OhmAlloy30

0.35

350

Copper-nickel--30

OhmAlloy35

0.35

350

Copper-nickel--34

OhmAlloy40

0.4

350

Copper-nickel--44

OhmAlloy49

0.5

400


Copper Nickel Alloy Heating Resistance Wire Cuni8 Technique Data

Normal composition%
Nickel45Manganese1
CopperBal.  

Typical Mechanical properties(1.0mm)
Yield strengthTensile StrengthElongation
MpaMpa%
25042025

Typical Physical properties
Density (g/cm3)8.9
Electrical resistivity at 20ºC (Ωmm2/m)0.49
Temperature factor of resistivity(20ºC~600ºC)X10-5/ºC -6
Conductivity coefficient at 20ºC (WmK)                 23
EMF vs Cu(μV/ºC )(0~100ºC )-43

Coefficient of thermal expansion
TemperatureThermal Expansion x10-6/K
20 ºC- 400ºC16

Specific heat capacity
Temperature20ºC
J/gK0.41
Melting point (ºC)1280
Max continuous operating temperature in air (ºC)400
Magnetic propertiesnon-magnetic

Corrosion resistance performance
AlloysWorking In atmosphere at 20ºC           Working at max temperature 200ºC
Air and oxygen contain
gases
gases with Nitrogengases with sulfur
oxidability
gases with sulfur
reductibility
carburization
OhmAlloy049goodbadbadbadbadgood

Style of supply
Alloys NameTypeDimension
OhmAlloy049WWireD=0.03mm~8mm
OhmAlloy049RRibbonW=0.4~40T=0.05~2.9mm
OhmAlloy049SStripW=8~200mmT=0.1~3.0
OhmAlloy049FFoilW=6~120mmT=0.005~0.1
OhmAlloy049BBarDia=8~100mmL=50~1000

Our Packing