China Nimonic / Haynes Allou 263 Uns N07263 Ws 2.4650 Sheet, Strip, Plate, Flat Bar, Wire, Tube and Forgings, Round Bar/Rod, Find details about China Alloy Steel Bar, Steel Bar from Nimonic / Haynes Allou 263 Uns N07263 Ws 2.4650 Sheet, Strip, Plate, Flat Bar, Wire, Tube and Forgings, Round Bar/Rod
Specifications
Alloy Name | Trade Name | UNS No. | British Specs | American Specs | German Specs | French Specs |
Alloy 263 | Nimonic 263 Haynes 263 | UNS N07263 | BS HR10 BS HR206 BS HR404 | AMS 5872 Sheet Strip and Plate AMS 5886 Bar and Forgings | WS 2.4650 |
Chemical Composition Limits | |||||||||
Weight% | Ni | Cr | Mn | Si | C | Al | Ag | B | Fe |
263 | Bal | 19-21 | 0.60 max | 0.40 max | 0.04-0.08 | 0.60 max | 0.0005 max | 0.005 max | 0.07 max |
Weight% | Cu | Mo | Co | Ti | Al+Ti | Pb | Bi | S | |
263 | 0.20 max | 5.6-6.1 | 19-21 | 1.90-2.40 | 2.40-2.8 | 0.0020 max | 0.0001 max | 0.007 max |
Material | Temp °C | Yield Strength 0.2% (Mpa) | Tensile Strength (Mpa) | Elongation % | Hardness HB |
Nimonic 263 Bar Solution Treated (AMS 5886/ BS HR10) | RT | - | - | - | 248 max |
Nimonic 263 Bar Heat Treated (AMS 5886 / BS HR10) | RT | 585 (typical) | 1004 (typical) | 45 | - |
Nimonic 263 Bar Heat Treated (AMS 5886/ BS HR10) | 780 | 403 (min) | 541 (min) | 12 | - |
Material | Temp °C | Yield Strength (Mpa) | Tensile Strength (Mpa) | Elongation % | Hardness HRC |
Nimonic 263 Sheet Solution Treated (AMS 5872 / BS HR206) | RT | - | - | - | 22.5 max |
Nimonic 263 Sheet Heat Treated (AMS 5872 / BS HR206 | RT | 580 (typical) | 973 (typical) | 39 - | |
Nimonic 263 Sheet Heat Treated (AMS 5872 / BS HR206 | 780 | 403 (min) | 541 (min) | 9 | - |
Alloy 263 can be welded using matching composition filler wire in both TIG and MIG forms. The recommended heat treatments for Nimonic 263 are as follows:
Extruded Bar:
Solution Treatment - 1150 °C for 1.5-2.5 hours + water quench
Ageing Treatment - 800 °C for 8 hours + air cool
(As per BS HR10 / AMS 5886)
Hot-rolled Sheet
Solution Treatment - 1150 °C for 0.5 hours + water quench or air cool
Ageing Treatment - 800 °C for 8 hours + air cool
(As per BS HR206/ AMS 5872)
Cold-rolled Sheet
Solution Treatment - 1150 °C for 3-10 mins + water quench or fluidized bed quenching
Ageing Treatment - 800 °C for 8 hours + air cool
(As per BS HR206 / AMS 5872)
Specifications:
UNS N07263 Werkstoff Nr. 2.4650 BS HR10 Rod and Bar BS HR 206 Plate, Sheet, Strip BS HR 404 Seamless Tube AECMA PrEn 2199 Bar AECMA PrEn 2200 Forgings AECMA PrEn 2201 Bar
AECMA PrEn 2202 Tube AECMA PrEn 2203 Sheet, Strip AECMA PrEn 2418 Plate
DIN 17750 Plate, Sheet, Strip DIN 17751 Pipe and Tube DIN 17752 Bar and Rod DIN 17753 Wire
DIN 17754 Forgings
AMS 5872 Sheet, Plate and Strip AMS 5886 Bar, Forgings, Rings AFNOR NCK 20 D
AIR 9165 Sheet, Plate, Rod, Bar and Forgings
MSRR 7035 MSRR 7036 GE B50A774A
Tradename's: Nicrofer 5120, Hastelloy C263 and Nimonic 263.