China High Level Homopolymer Polypropylene PP Raw Material PP Granules, Find details about China PP Raw Material, PP Resin from High Level Homopolymer Polypropylene PP Raw Material PP Granules
Item | Parameter | Test Standard |
MFR (2.16kg) | 3-5g/10min | GB/T 3682 |
Isotacticity | ≥ 97% | GB/T 2412 |
Tensile strength | >33Mpa | GB/T 1040.2 |
Ash content | ≤0.03% | GB/T 9345.1 |
Notched IZOD impact strength at 23 ºC | ≥3 kJ/m² | GB/T 1043.1 |
Flexural Modulus | >1300 Mpa | GB/T 9341 |
Yellow index | ≤4 | HG/T 3862 |
Item | Parameter | Test Standard |
MFR (2.16kg) | 14-19g/10min | GB/T 3682 |
Isotacticity | ≥ 97% | GB/T 2412 |
Tensile strength | >33Mpa | GB/T 1040.2 |
Ash content | ≤0.03% | GB/T 9345.1 |
Notched IZOD impact strength at 23 ºC | ≥3 kJ/m² | GB/T 1043.1 |
Flexural Modulus | >1300 Mpa | GB/T 9341 |
Yellow index | ≤4 | HG/T 3862 |
Item | Parameter | Test Standard |
MFR (2.16kg) | 26-30g/10min | GB/T 3682 |
Isotacticity | ≥ 97% | GB/T 2412 |
Tensile strength | >33Mpa | GB/T 1040.2 |
Ash content | ≤0.03% | GB/T 9345.1 |
Notched IZOD impact strength at 23 ºC | ≥3 kJ/m² | GB/T 1043.1 |
Flexural Modulus | >1300 Mpa | GB/T 9341 |
Yellow index | ≤4 | HG/T 3862 |
Item | Parameter | Test Standard |
MFR (2.16kg) | >65/10min | GB/T 3682 |
Isotacticity | ≥ 98% | GB/T 2412 |
Tensile strength | >36Mpa | GB/T 1040.2 |
Ash content | ≤0.03% | GB/T 9345.1 |
Notched IZOD impact strength at 23 ºC | ≥1.5kJ/m² | GB/T 1043.1 |
Flexural Modulus | >1300 Mpa | GB/T 9341 |
Yellow index | ≤4 | HG/T 3862 |