China Reaction Bonded Silicon Carbide Tile Bricks, Find details about China Silicon Carbide Brick, Silicon Carbide Tile from Reaction Bonded Silicon Carbide Tile Bricks
Item | Unit | Data |
Temperature of application | ºC | 1380ºC |
Density | G/cm3 | >3.05 |
Open porosity | % | <0.1 |
Bending strength -A | Mpa | 250 (20ºC) |
Bending strength -B | MPa | 280 (1200ºC ) |
Modulus of elasticity-A | GPa | 330(20ºC) |
Modulus of elasticity -B | GPa | 300 ( 1200ºC ) |
Thermal conductivity | W/m.k | 45 (1200ºC ) |
Coefficient of thermal expansion | K-1 ×10-6 | 4.5 |
Rigidity | / | 13 |
Acid-proof alkaline | / | excellent |