China Excellent Insulation Performance Heat Shrink Sleeve for Busbar, Find details about China Heat Shrink Sleeve, Heat Shrink Sleeve for Busbar from Excellent Insulation Performance Heat Shrink Sleeve for Busbar
Property | Typical Data | Test Method |
Tensile strength | ≥8.0MPa | ASTM D 2671 |
Elongation at break | ≥300% | ASTM D 2671 |
Tensile strength after heat ageing | ≥6.9MPa | 130ºC×168h |
Elongation after heat ageing | ≥100% | 130ºC×168h |
Longitudinal change | -8%~+8% | ASTM D 2671 |
Flammability(Oxygen index) | ≥28 | GB/T 2406 |
Heat Shock | No cracking | JB 7829 supplement D |
Dielectric Strength | ≥20kv/mm | ASTM D 149 |
Shore A Hardness | ≤90 | GB2411 |
Volume resistivity | ≥1014Ω.cm | IEC 60093 |
Size(mm) | As supplied(mm) D | After recovered(mm) | Standard length | |
Inner diameter d | Wall thickness w | (M/spool) | ||
Φ30/15 | ≥30 | ≤15 | 4.0±0.30 | 15 |
Φ40/20 | ≥40 | ≤20 | 4.0±0.30 | 15 |
Φ50/25 | ≥50 | ≤25 | 4.0±0.30 | 15 |
Φ65/33 | ≥65 | ≤33 | 4.0±0.30 | 15 |
Φ75/38 | ≥75 | ≤38 | 4.0±0.30 | 15 |
Φ85/43 | ≥85 | ≤43 | 4.0±0.30 | 15 |
Φ100/50 | ≥100 | ≤50 | 4.0±0.30 | 15 |
Φ120/60 | ≥120 | ≤60 | 4.0±0.30 | 15 |
Φ150/75 | ≥150 | ≤75 | 4.0±0.30 | 15 |
Φ180/90 | ≥180 | ≤90 | 4.0±0.30 | 15 |
Φ210/105 | ≥210 | ≤105 | 4.0±0.30 | 15 |
Φ230/115 | ≥230 | ≤115 | 4.0±0.30 | 15 |
Φ250/125 | ≥250 | ≤125 | 4.0±0.30 | 15 |
Φ300/150 | ≥300 | ≤150 | 4.0±0.30 | 15 |