China SBR 1502 1716 (styrene butadiene rubber), Find details about China Styrene Butadiene Rubber, Styrene Butadiene Rubber Sbr 1502 1716 from SBR 1502 1716 (styrene butadiene rubber)
SBR 1Specification Values(GB/T12824-2002) | |||||
Item |
Property | Test Method | |||
A | B | C | |||
Volatile matter % | ≤0.60 | ≤0.75 | ≤0.90 | GB/T 6737-1997 | |
Ash % | ≤0.50 | GB/T 4498-1997 A | |||
Organic acid % | 4.50-6.75 | GB/T 8657-2000 A | |||
Soap % | ≤0.50 | ||||
Bound styrene % | 22.5-24.5 | GB/T 8658-1998 | |||
Mooney viscosity 50ML(1+4)100 | 45-55 | 44-56 | GB/T 1232.1-2000 | ||
Compound 50ML(1+4)100 | ≤93 | ||||
300% 145MPa, 300%Modulus |
25min | M±2.0 | M±2.5 | GB/T 8656-1998 A | |
35min | 20.6±2.0 | 20.6±2.5 | |||
50min | 21.5±2.0 | 21.5±2.5 | |||
Tensile strength (145,35min), MPa | ≥25.5 | ≥24.5 | |||
Elongation (145,35min),% | ≥340 | ≥330 |
SBR 2 Specification (SH/T 1626-2005) | |||||
Item |
Property | Test Method | |||
A | B | C | |||
Volatile matter% m/m | ≤0.60 | ≤0.80 | ≤1.00 | GB/T 6737-1997 | |
Ash% (m/m) | ≤0.50 | GB/T 4498-1997 | |||
Organic acid %m/m | 3.90-5.70 | GB/T 8657-2000 | |||
Soap %m/m | ≤0.50 | ||||
Bound styrene% m/m | 22.5-24.5 | GB/T 8658-1998 | |||
Oil %m/m | 25.3-29.3 | 24.3-30.3 | SH/T 1718-2002 | ||
Mooney viscosity ML(1+4)100 | 44-54 | 43-55 | 42-56 | GB/T 1232.1-2000 | |
Compound ML(1+4)100 | ≤70 | GB/T 1232.1-2000 ASTM IRB No.7 | |||
300%Modulus (145),MPa | 25min | 9.8-13.8 | 9.3-14.3 |
GB/T 8656-1998 ASTM IRB No.7 GB/T 528-1998 I |
|
35min | 12.1-16.1 | 11.6-16.6 | |||
50min | 13.0-17.0 | 12.5-17.5 | |||
145,35min), MPa Tensile strength |
≥19.4 | ≥18.4 | |||
(145,35min), % Elongation |
≥380 | ≥370 |