Platinum Cure Pad Printing Silicone Rubber

China Platinum Cure Pad Printing Silicone Rubber, Find details about China Silicone Rubber, Silicone Pads from Platinum Cure Pad Printing Silicone Rubber

Model NO.
HY933
HS Code
39100000
Model NO.
HY933
HS Code
39100000

platinum cure pad printing silicone rubber 
HY-933 is a kind of room temperature vulcanized silicone rubber in addition type. It's generally named as two part silicone rubber, 9:1 Part A is a flowable liquid, part B is the curing agent or catalyst. It's mainly used for printing pads making.

The silicon pad is a carrier which transfers the patterns from the steel plate onto the products' surface. It has the
advantage of good printing effects, fine quality, good resilience, and without any impurity.

Application
HY-933 silicone rubber is used for is mainly use for printing irregular patterns on plastic toys,shampoo, pen, glass,electroplating products,electroplating toys and trade marks artwork gifts, and stationery and so on.
 
Technical Parameters 

ModelColorMixing
ratio 
(%)
Pot life
(mins,
under 25ºC)
Curing 
time h
(under
 25ºC)
Hardness 
(Shore A )
Tensile-
strength
 (MPa)
Tear-
strength
 (kN/m)
Viscosity
(After A/B
 mixed,mPa.s)
Shrinkage
rate (%)
Elongation
(%)
HY-933Red
White
 
9:130-404-633±2 4.5±0.5 
22±2
 
 
10000-15000
 
≤0.3%  350±50

 
Operation instructions
Step 1: prepare the original silicone pad molds
Make sure your original molds smooth and Clear .
Step2: Mix part A liquid silicone and silicone oil
Usually the original hardness of the silicone pad is around 28 shore A , our customer will add silicone oil by adjust the hardness , when adding 2% silicone oil , the hardness will reduce 2 shore A , for example 933 silicone is 28 shore A , if you require hardness of 25 shore A for printing , then add 6% silicone oil .The percentage of silicone oil added should not more than 30% . Adding silicone oil into the liquid silicone and mix it evenly
Step3:Add 10G part B catalyst into the mixture of liquid silicone with silicone oil and mix them evenly.
*Notes: After the Step 2 by adding and mix the silicone oil evenly ,add 10G catalyst into the mixture (10% is the weight for the totally mixture of liquid silicone and silicone oil ) and mix them evenly .
         1.Weigh the exactly weight by electronic weight..
If not , for example add too much catalyst , the operation time will be too fast to operate ,which will cause inconvenience to operate .
         2.Mixture should stir evenly.
Otherwise the silicon rubber will be partly solidified and this will give birth to difficulties in your final operation. What's more, the finished molds will meet a short life. All of these will cause a waste of silicon rubber.
Step4: Vacuum pumping
Without exception, this step takes less than 10 minutes. Otherwise, it will cause cross linking reaction, and no more further steps will be available.
Step 5: Pouring the mixture into the original mold
*Notes:1. Put an wooden board on the surface of the silicone pad and set an hole on the board to make sure the board will closely stick on the pad .
        2.Wait till the silicone pad totally cured before put into production.
      
Package
20KG/drum vacuum packing for part A +1kg/ bottle catalyst for part B
 
Shelf life
Eight to Ten(8-10) months when stored under dry and cool place by original package under 25ºC.