Plate Type | Non-ablation thermal-negative type |
Application | High grade commercial and newspaper printing |
Substrate | Electrolyte graining and Anodized AL substrate |
Thickness | 0.15mm / 0.30mm |
Spectrum scope | 800-850nm |
Platesetter | Various dominant thermal platesetters in the market |
Low-energy imaging | 130~150mJ/m² |
The period of latent image stabilization | ≤7days |
Recommended screen method | 1~99 @200Lpi AM/20u FM and mixture |
The paper number of startup | <50 sheets |
Safety Light | 1 hour under fluorescent lamp, no direct irradiation with natural light, 4 hours under yellow light |
Processing | Without processing,directly on press |
Run Length | 100,000 impressions,actual run length depends on printing conditions |