Fiberglass Core PARA-Aramid Rope

China Fiberglass Core PARA-Aramid Rope, Find details and Price about China Fiberglass Core Kevlar Yarn, Glass Fiber Reinforced Kevlar Yarn from Fiberglass Core PARA-Aramid Rope

Model NO.
XGPFE245/1
Pattern
Raw
Type
Twisted Yarn
Coarseness
Medium Yarn
Structure
Ring Spun Yarn
Model
Xgpfe245/1
Color
Light Yellow
Fiber Type
PARA-Aramid
Content of Aramid
50%
Yarn Density
245tex
Yarn Diameter
0.76mm
Yarn Length
4081m(+/-5%)
Breaking Force
8516cn
Oxygen Index
>28%
Net Weight
3.00kg+/-0.05kg
Trademark
XIANGU
Transport Package
12kg Per Carton
Specification
ROHS
Origin
Guangdong
HS Code
54021190
Model NO.
XGPFE245/1
Pattern
Raw
Type
Twisted Yarn
Coarseness
Medium Yarn
Structure
Ring Spun Yarn
Model
Xgpfe245/1
Color
Light Yellow
Fiber Type
PARA-Aramid
Content of Aramid
50%
Yarn Density
245tex
Yarn Diameter
0.76mm
Yarn Length
4081m(+/-5%)
Breaking Force
8516cn
Oxygen Index
>28%
Net Weight
3.00kg+/-0.05kg
Trademark
XIANGU
Transport Package
12kg Per Carton
Specification
ROHS
Origin
Guangdong
HS Code
54021190
Fiberglass Core Para-aramid Rope

1 thread of fiberglass filament reinforced core para-aramid fiber twisted yarn is made of fiberglass filament as core material with high strength and high modulus 1414 para aramid staple winding outer. Para-aramid fiber is evenly wrapped in glass fiber through spinning process. The surface has a low twist and the single yarn density is approximately 245 tex. This kind of yarn has both the high strength,high modulus and high toughness of fiberglass and para-aramid fiber.Good chemical resistance,acid and alkali,anti-aging,fire retardant properties.Generally used to produce large-scale ships ropes,life-saving rescue ropes,fire ropes and other products.

SPECIFICATIONS:
Model:XGPFE245/1
Color:Light yellow
Fiber material:Para-aramid &fiberglass
Yarn density:245tex
Yarn diameter:0.76mm
Yarn length:4081m/kg
Breaking force:8516CN
Breaking gravity:8.69kg
Oxygen Index:>28%
Twist:30-50Pc/m
Net weight:3.00kg+/-0.05kg

STORAGE:
The fiberglass filament reinforced para aramid twisted yarn should be keep dry in their original bags and stored in a suitable place,preferably at room temperature with 35-65% relative humidity.Avoid the sun, rain and fire.

PACKAGING:
Fiberglass Core PARA-Aramid Rope



PRODUCT DETAIL IMAGES:
Fiberglass Core PARA-Aramid Rope
Fiberglass Core PARA-Aramid Rope
Fiberglass Core PARA-Aramid Rope
Fiberglass Core PARA-Aramid Rope
Fiberglass Core PARA-Aramid Rope