China Reusable Plastic Hollow Board Concrete Mould Formwork for Building Construction Site, Find details about China Building Material, Scaffolding from Reusable Plastic Hollow Board Concrete Mould Formwork for Building Construction Site
Test items | Test method | Result | |
Bending test | Refer to JG/T 418-2013,section 7.2.5 & GB/T9341-2008 | Bending strength | 25.8MPa |
Flexural modulus | 1800MPa | ||
Softening temperature of VEKA | Refer to JG/T 418-2013, section 7.2.6 & GB/T 1633-2000 method BO5 | 75.7 °C |