China Liquid, Latency, Silicon Powder Thermocuring Casting Resin System for Transformer, Find details about China Epoxy Resin, Cast Resin from Liquid, Latency, Silicon Powder Thermocuring Casting Resin System for Transformer
TD-9005A | Appearance | Vision | Transparent | |||
Viscosity | at 40°C | ISO 2555: 1989 | mpas Pas | 700-800 | ||
(Measurements with Brookfield Gel Instrument) | ||||||
Density | at 25°C | ISO 2811-2:1997 | g/cm3 | 1.05 - 1.12 |
TD-9005B | Appearance | Vision | Light Yellow | |||
Viscosity | at 40°C | ISO 2555: 1989 | mpas Pas | 250-350 | ||
(Measurements with Brookfield Gel Instrument) | ||||||
Density | at 25°C | ISO 2811-2:1997 | g/cm3 | 1.08 - 1.10 |
Tensile strength ISO | R | 527 | N/mm2 | 60 - 70 | ||
Elongation at break ISO | R | 527 | % | 1.5 - 1.8 | ||
Flexural Strength | ISO | 178:2001 | MPa | 110 - 130 | ||
Surface Strain | % | 1.5 - 1.7 | ||||
Compressive strength | ISO | 604 | N/mm2 | 185 - 190 | ||
Double Torsion Test | PM 216-1989 | |||||
Critical stress intensity factor (KIC) | MPa m1/2 2.0 - 2.4 | |||||
Specific fracture energy(GIC) | J/m2 | 470 - 550 | ||||
Tg(GTT) Glass Transition Temperature | ISO 11357-2: 1999 | ºC | 80 - 85 | |||
Coefficient of linear thermal expansion | ISO 11359:1999 | |||||
Lower than average value of Tg | ppm/K | 40 - 43 | ||||
Water Absorption(Specimen:50*50*4cm3) | ISO 62 | |||||
60 min at 100°C | % | 0.15-0.20 | ||||
Density | g/cm3 | 1.05-1.12 |