Magnesium Oxide Crucible

China Magnesium Oxide Crucible, Find details about China Magnesia Crucible, High Purity Magnesia Pot from Magnesium Oxide Crucible

Model NO.
GT-165
Finsh
Bore, Slot
Application
Thermal Analysis or Firing
Feature
Long Time Materials
Material
Zirconia
Trademark
shangtao
Transport Package
Plywood Case
Specification
Rohs
Origin
Shanghai, China
HS Code
6091900000
Model NO.
GT-165
Finsh
Bore, Slot
Application
Thermal Analysis or Firing
Feature
Long Time Materials
Material
Zirconia
Trademark
shangtao
Transport Package
Plywood Case
Specification
Rohs
Origin
Shanghai, China
HS Code
6091900000
Magnesium Oxide Crucible


Gongtao company can make various crucibles and saggers made of high alumina, with different shapes. And we can also custom based on the requirement.

Series:
Alumina ceramic crucible
Corundum ceramic crucible
Arc alumina crucibles(high form alumina crucibles)
Cylindrical alumina ceramic crucibles
Rectangular crucibles
Special shaped crucibles
Alumina saggers
Zirconia crucible
Mgo crucible

Purpose: Main purpose of crucible and sagger is as a container for analysis and firing of material and product applied in various industries. For example: Analysis of coal, melting of the metal, analysis and firing of chemical raw materials, analysis and melting of glass, analysis and firing of rare earth materials and mineral, firing of high temperature items such as ceramic products and melting of single-crystal raw materials.

Use: Under normal circumstances, firstly put the items which need to be analyzed and fired into the crucible or sagger. Then heat. The speed of heating and drop in temperature are according to the characteristics of equipment and products, fast or slow. Because of the thermal expansion of raw material which the crucibles and saggers are made of, too quick heating or cooling will easily lead to cracking of the crucibles and saggers. The best way is slowing down, which can prolong the life of them.

& Electrical Characteristics

Unit

MgO

Contents

%

95 99.5

density

g/cm3

3.56

hardness

Mohs'

6

liner thermal expansion

/oC

(40o to 250o)

8.6 x 10-6

work temperature

oC

2400

flexual strength

MPa

84

compressure strength

MPa

14

fracture strength (5 distance)

MPa

125

thermal conductivity

W/m.k

15.9-42

Volume resistivity (100 oC)

 

>1012